{"title":"少量添加镁的Al-7Si-0.3Mg合金高温干滑动磨损特性","authors":"M. S. Prabhudev, S. A. Kori","doi":"10.1080/17515831.2021.1945861","DOIUrl":null,"url":null,"abstract":"ABSTRACT In this paper, effect of minor additions of magnesium content in the form of master alloys on the high-temperature dry sliding wear behaviour for A356 alloy has been reported. Alloy composition, normal pressures and sliding distances on A356 alloy at constant temperature of 300°C was studied. The cast alloys and worn surfaces were characterized by SEM/EDX microanalysis. The results indicate that the wear rate of A356 alloy increases with an increase in normal pressures and sliding distances in all the cases and decreases when 0.7% Mg is added to A356 alloy. The decrease in wear rate after the addition of Mg is mainly due to changes in microstructure which lead to improvement in mechanical properties. Further, worn surface study indicates that the formation of iron-rich oxide layer between the mating surfaces during sliding improves sliding wear performance. GRAPHICAL ABSTRACT","PeriodicalId":23331,"journal":{"name":"Tribology - Materials, Surfaces & Interfaces","volume":null,"pages":null},"PeriodicalIF":1.6000,"publicationDate":"2021-07-14","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1080/17515831.2021.1945861","citationCount":"0","resultStr":"{\"title\":\"Dry sliding wear characteristics of Al-7Si-0.3Mg alloy with minor additions of magnesium at high temperature\",\"authors\":\"M. S. Prabhudev, S. A. Kori\",\"doi\":\"10.1080/17515831.2021.1945861\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"ABSTRACT In this paper, effect of minor additions of magnesium content in the form of master alloys on the high-temperature dry sliding wear behaviour for A356 alloy has been reported. Alloy composition, normal pressures and sliding distances on A356 alloy at constant temperature of 300°C was studied. The cast alloys and worn surfaces were characterized by SEM/EDX microanalysis. The results indicate that the wear rate of A356 alloy increases with an increase in normal pressures and sliding distances in all the cases and decreases when 0.7% Mg is added to A356 alloy. The decrease in wear rate after the addition of Mg is mainly due to changes in microstructure which lead to improvement in mechanical properties. Further, worn surface study indicates that the formation of iron-rich oxide layer between the mating surfaces during sliding improves sliding wear performance. GRAPHICAL ABSTRACT\",\"PeriodicalId\":23331,\"journal\":{\"name\":\"Tribology - Materials, Surfaces & Interfaces\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":1.6000,\"publicationDate\":\"2021-07-14\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://sci-hub-pdf.com/10.1080/17515831.2021.1945861\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Tribology - Materials, Surfaces & Interfaces\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1080/17515831.2021.1945861\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"MATERIALS SCIENCE, COATINGS & FILMS\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Tribology - Materials, Surfaces & Interfaces","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1080/17515831.2021.1945861","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"MATERIALS SCIENCE, COATINGS & FILMS","Score":null,"Total":0}
引用次数: 0

摘要

本文研究了以中间合金形式添加少量镁元素对A356合金高温干滑动磨损性能的影响。研究了A356合金在300℃恒温下的合金成分、法向压力和滑动距离。采用SEM/EDX显微分析对铸态合金和磨损表面进行了表征。结果表明:在所有情况下,A356合金的磨损率均随法向压力和滑动距离的增加而增加,当添加0.7% Mg时,磨损率降低;添加Mg后磨损率的降低主要是由于微观组织的改变导致力学性能的改善。此外,磨损表面研究表明,在滑动过程中,在配合表面之间形成的富铁氧化层提高了滑动磨损性能。图形抽象
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Dry sliding wear characteristics of Al-7Si-0.3Mg alloy with minor additions of magnesium at high temperature
ABSTRACT In this paper, effect of minor additions of magnesium content in the form of master alloys on the high-temperature dry sliding wear behaviour for A356 alloy has been reported. Alloy composition, normal pressures and sliding distances on A356 alloy at constant temperature of 300°C was studied. The cast alloys and worn surfaces were characterized by SEM/EDX microanalysis. The results indicate that the wear rate of A356 alloy increases with an increase in normal pressures and sliding distances in all the cases and decreases when 0.7% Mg is added to A356 alloy. The decrease in wear rate after the addition of Mg is mainly due to changes in microstructure which lead to improvement in mechanical properties. Further, worn surface study indicates that the formation of iron-rich oxide layer between the mating surfaces during sliding improves sliding wear performance. GRAPHICAL ABSTRACT
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Tribology - Materials, Surfaces & Interfaces
Tribology - Materials, Surfaces & Interfaces MATERIALS SCIENCE, COATINGS & FILMS-
CiteScore
2.80
自引率
0.00%
发文量
15
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信