Xiaoli Shi, Lu Zhang, Yan-fei Liu, Jinyu Wang, Gui Zhang, Haiping Qi, Wanqian Zhang, Deyuan Zhang, Jin Wang
{"title":"铁基生物可吸收支架的慢性毒性和致癌性研究","authors":"Xiaoli Shi, Lu Zhang, Yan-fei Liu, Jinyu Wang, Gui Zhang, Haiping Qi, Wanqian Zhang, Deyuan Zhang, Jin Wang","doi":"10.1515/ntrev-2022-0507","DOIUrl":null,"url":null,"abstract":"Abstract Fe-based stents have been made a figure in biodegradable stents by their good mechanical capacity and biocompatibility, appropriate strength–ductility combination. Although the iron corrosion rate was not ideal, which had been optimized by iron alloy and polymer coating introduction. As a long-term implanted biodegradable material, the real concern about iron-based stents mainly laid in long-term biosafety. In this work, rats were used as an animal model to study the chronic toxicity and carcinogenicity of iron-based stents. Two years later, the changes in body weight and the physiological status during the experiment were monitored, and the blood routine and blood analysis combined with the health of major organs and histopathological tests were performed. The results demonstrated that there was no significant difference compared with the control group (316L SS) in body weight, blood routine index, blood biochemical index, and carcinogenic rate that further confirmed the biosafety of iron-based material.","PeriodicalId":18839,"journal":{"name":"Nanotechnology Reviews","volume":" ","pages":""},"PeriodicalIF":6.1000,"publicationDate":"2023-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Study on the chronic toxicity and carcinogenicity of iron-based bioabsorbable stents\",\"authors\":\"Xiaoli Shi, Lu Zhang, Yan-fei Liu, Jinyu Wang, Gui Zhang, Haiping Qi, Wanqian Zhang, Deyuan Zhang, Jin Wang\",\"doi\":\"10.1515/ntrev-2022-0507\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Abstract Fe-based stents have been made a figure in biodegradable stents by their good mechanical capacity and biocompatibility, appropriate strength–ductility combination. Although the iron corrosion rate was not ideal, which had been optimized by iron alloy and polymer coating introduction. As a long-term implanted biodegradable material, the real concern about iron-based stents mainly laid in long-term biosafety. In this work, rats were used as an animal model to study the chronic toxicity and carcinogenicity of iron-based stents. Two years later, the changes in body weight and the physiological status during the experiment were monitored, and the blood routine and blood analysis combined with the health of major organs and histopathological tests were performed. The results demonstrated that there was no significant difference compared with the control group (316L SS) in body weight, blood routine index, blood biochemical index, and carcinogenic rate that further confirmed the biosafety of iron-based material.\",\"PeriodicalId\":18839,\"journal\":{\"name\":\"Nanotechnology Reviews\",\"volume\":\" \",\"pages\":\"\"},\"PeriodicalIF\":6.1000,\"publicationDate\":\"2023-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Nanotechnology Reviews\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.1515/ntrev-2022-0507\",\"RegionNum\":3,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"CHEMISTRY, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Nanotechnology Reviews","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1515/ntrev-2022-0507","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"CHEMISTRY, MULTIDISCIPLINARY","Score":null,"Total":0}
Study on the chronic toxicity and carcinogenicity of iron-based bioabsorbable stents
Abstract Fe-based stents have been made a figure in biodegradable stents by their good mechanical capacity and biocompatibility, appropriate strength–ductility combination. Although the iron corrosion rate was not ideal, which had been optimized by iron alloy and polymer coating introduction. As a long-term implanted biodegradable material, the real concern about iron-based stents mainly laid in long-term biosafety. In this work, rats were used as an animal model to study the chronic toxicity and carcinogenicity of iron-based stents. Two years later, the changes in body weight and the physiological status during the experiment were monitored, and the blood routine and blood analysis combined with the health of major organs and histopathological tests were performed. The results demonstrated that there was no significant difference compared with the control group (316L SS) in body weight, blood routine index, blood biochemical index, and carcinogenic rate that further confirmed the biosafety of iron-based material.
期刊介绍:
The bimonthly journal Nanotechnology Reviews provides a platform for scientists and engineers of all involved disciplines to exchange important recent research on fundamental as well as applied aspects. While expert reviews provide a state of the art assessment on a specific topic, research highlight contributions present most recent and novel findings.
In addition to technical contributions, Nanotechnology Reviews publishes articles on implications of nanotechnology for society, environment, education, intellectual property, industry, and politics.