{"title":"电沉积法降低电镀工业废水中铜的金属离子含量","authors":"Tangke Veronika, Bohari Yusuf, R. Gunawan","doi":"10.30872/JKM.V16I1.415","DOIUrl":null,"url":null,"abstract":"The reduction of copper concentration in the electroplating industry wastewater by electrodeposition method by means of Atomic Absorption Spectrophotometer (AAS). The result of research showed that degradation and is big of elimination percent of copper metal have with the effect of time contact and voltage at optimum hence in getting results of final concentration of iron (Fe) successive plate 4,02 ppm and 2,84 ppm of concentration early 35,86 ppm and elimination percent of exclusion at optimum parameter in getting result successive 88,403 % and 92,069 %. While the results of the final concentration of Aluminium (Al) successive plate 2,38 ppm dan 2,22 ppm of concentration early 35,86 ppm and elimination percent of exclusion at optimum parameter in getting result successive 93,363 % dan 93,814%.","PeriodicalId":31725,"journal":{"name":"Jurnal Kimia Mulawarman","volume":" ","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2018-11-29","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"DECREASED LEVEL OF METAL IONS OF COPPER (CU) IN THE ELECTROPLATING INDUSTRY WASTE WATER USING ELECTRODEPOSITION METHOD\",\"authors\":\"Tangke Veronika, Bohari Yusuf, R. Gunawan\",\"doi\":\"10.30872/JKM.V16I1.415\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The reduction of copper concentration in the electroplating industry wastewater by electrodeposition method by means of Atomic Absorption Spectrophotometer (AAS). The result of research showed that degradation and is big of elimination percent of copper metal have with the effect of time contact and voltage at optimum hence in getting results of final concentration of iron (Fe) successive plate 4,02 ppm and 2,84 ppm of concentration early 35,86 ppm and elimination percent of exclusion at optimum parameter in getting result successive 88,403 % and 92,069 %. While the results of the final concentration of Aluminium (Al) successive plate 2,38 ppm dan 2,22 ppm of concentration early 35,86 ppm and elimination percent of exclusion at optimum parameter in getting result successive 93,363 % dan 93,814%.\",\"PeriodicalId\":31725,\"journal\":{\"name\":\"Jurnal Kimia Mulawarman\",\"volume\":\" \",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2018-11-29\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Jurnal Kimia Mulawarman\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.30872/JKM.V16I1.415\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Kimia Mulawarman","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.30872/JKM.V16I1.415","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

原子吸收分光光度法(AAS)电沉积法降低电镀工业废水中铜的浓度。研究结果表明,铜金属的降解和消除率大受接触时间和最佳电压的影响,因此获得的铁(Fe)连续板的终浓度为4,02 ppm和2,84 ppm,早期浓度为35、86 ppm和最佳参数的消除率分别为88,403 %和92,069 %。而铝(Al)连续板的最终浓度为2,38 ppm、2,22 ppm、2,35 ppm、86 ppm和排除率在最优参数下得到的结果为连续板的93,363%和93,814%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
DECREASED LEVEL OF METAL IONS OF COPPER (CU) IN THE ELECTROPLATING INDUSTRY WASTE WATER USING ELECTRODEPOSITION METHOD
The reduction of copper concentration in the electroplating industry wastewater by electrodeposition method by means of Atomic Absorption Spectrophotometer (AAS). The result of research showed that degradation and is big of elimination percent of copper metal have with the effect of time contact and voltage at optimum hence in getting results of final concentration of iron (Fe) successive plate 4,02 ppm and 2,84 ppm of concentration early 35,86 ppm and elimination percent of exclusion at optimum parameter in getting result successive 88,403 % and 92,069 %. While the results of the final concentration of Aluminium (Al) successive plate 2,38 ppm dan 2,22 ppm of concentration early 35,86 ppm and elimination percent of exclusion at optimum parameter in getting result successive 93,363 % dan 93,814%.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
3
审稿时长
16 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信