{"title":"静电纺丝法制备壳聚糖-聚氧聚乙烯-木薯粉纳米纤维","authors":"Riesca Ayu Kusuma Wardhani, L. Asri, M. Nasir, B. S. Purwasasmita","doi":"10.17977/UM016V3I12019P001","DOIUrl":null,"url":null,"abstract":"Nanofibers have been prepared from the mixture of chitosan, polyethylene oxide (PEO) and Colocasia esculenta flour (CE flour) by using the electrospinning method. Two different nanofibers were formulated, containing chitosan-PEO and chitosan-PEO-CE flour. The higher concentration of PEO (3%chitosan-6%PEO) (w/v) resulted in more uniform chitosan-PEO electrospun nanofibers without beads. Chitosan-PEO-CE flour was prepared by addition of colloidal CE flour into the solution containing 3%chitosan-6%PEO with variation of the CE flour concentration of 5, 15 and 25% (w/v). Scanning Electron Microscopy demonstrated that the average diameter of chitosan-PEO nanofibers was 128±41 nm, whereas the diameter of chitosan-PEO-CE flour nanofibers was 159±45 nm. The diameters of nanofibers increased with the increase of CE flour content. Fourier transform infrared spectra demonstrate the presence characteristic peaks of chitosan, PEO and CE flour.","PeriodicalId":16315,"journal":{"name":"Journal of Mechanical Engineering Science and Technology","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-08-13","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"6","resultStr":"{\"title\":\"Preparation of Chitosan-Polyethylene Oxide-Colocasia esculenta Flour Nanofibers using Electrospinning Method\",\"authors\":\"Riesca Ayu Kusuma Wardhani, L. Asri, M. Nasir, B. S. Purwasasmita\",\"doi\":\"10.17977/UM016V3I12019P001\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Nanofibers have been prepared from the mixture of chitosan, polyethylene oxide (PEO) and Colocasia esculenta flour (CE flour) by using the electrospinning method. Two different nanofibers were formulated, containing chitosan-PEO and chitosan-PEO-CE flour. The higher concentration of PEO (3%chitosan-6%PEO) (w/v) resulted in more uniform chitosan-PEO electrospun nanofibers without beads. Chitosan-PEO-CE flour was prepared by addition of colloidal CE flour into the solution containing 3%chitosan-6%PEO with variation of the CE flour concentration of 5, 15 and 25% (w/v). Scanning Electron Microscopy demonstrated that the average diameter of chitosan-PEO nanofibers was 128±41 nm, whereas the diameter of chitosan-PEO-CE flour nanofibers was 159±45 nm. The diameters of nanofibers increased with the increase of CE flour content. Fourier transform infrared spectra demonstrate the presence characteristic peaks of chitosan, PEO and CE flour.\",\"PeriodicalId\":16315,\"journal\":{\"name\":\"Journal of Mechanical Engineering Science and Technology\",\"volume\":\"1 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2019-08-13\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"6\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Mechanical Engineering Science and Technology\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.17977/UM016V3I12019P001\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Mechanical Engineering Science and Technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17977/UM016V3I12019P001","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 6

摘要

以壳聚糖、聚氧聚乙烯(PEO)和土芋粉(CE)为原料,采用静电纺丝法制备了纳米纤维。制备了壳聚糖- peo和壳聚糖- peo - ce粉两种不同的纳米纤维。较高的PEO浓度(3%壳聚糖-6%PEO) (w/v)使壳聚糖-PEO静电纺纳米纤维更均匀,无珠。将胶体CE粉加入到含有3%壳聚糖-6% peo的溶液中,CE粉的浓度分别为5%、15%和25% (w/v),制备了壳聚糖- peo -CE粉。扫描电镜结果表明,壳聚糖- peo纳米纤维的平均直径为128±41 nm,壳聚糖- peo - ce面粉纳米纤维的平均直径为159±45 nm。随着CE粉含量的增加,纳米纤维的直径增大。傅里叶变换红外光谱显示壳聚糖、PEO和CE粉的特征峰存在。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Preparation of Chitosan-Polyethylene Oxide-Colocasia esculenta Flour Nanofibers using Electrospinning Method
Nanofibers have been prepared from the mixture of chitosan, polyethylene oxide (PEO) and Colocasia esculenta flour (CE flour) by using the electrospinning method. Two different nanofibers were formulated, containing chitosan-PEO and chitosan-PEO-CE flour. The higher concentration of PEO (3%chitosan-6%PEO) (w/v) resulted in more uniform chitosan-PEO electrospun nanofibers without beads. Chitosan-PEO-CE flour was prepared by addition of colloidal CE flour into the solution containing 3%chitosan-6%PEO with variation of the CE flour concentration of 5, 15 and 25% (w/v). Scanning Electron Microscopy demonstrated that the average diameter of chitosan-PEO nanofibers was 128±41 nm, whereas the diameter of chitosan-PEO-CE flour nanofibers was 159±45 nm. The diameters of nanofibers increased with the increase of CE flour content. Fourier transform infrared spectra demonstrate the presence characteristic peaks of chitosan, PEO and CE flour.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
6
审稿时长
24 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信