影响正畸托槽与瓷的剪切粘结强度的因素。

B M Bourke, W P Rock
{"title":"影响正畸托槽与瓷的剪切粘结强度的因素。","authors":"B M Bourke,&nbsp;W P Rock","doi":"10.1093/ortho/26.4.285","DOIUrl":null,"url":null,"abstract":"<p><p>The aim of this investigation was to establish a regime for orthodontic bonding to feldspathic porcelain, which ensures adequate bond strength (6-8 MPa) with minimal damage on debond and consisted of an ex vivo investigation measuring the effects of porcelain surface preparation and thermocycling on shear bond strength of orthodontic brackets. One-hundred-and-twenty feldspathic porcelain bonded crown surfaces were divided into 12 equally-sized groups to assess the effects of: (1) glaze removal, (2) application of hydrofluoric acid, phosphoric acid, or omission of acid treatment, and (3) silane priming upon the bond strength of premolar brackets bonded with Right-on (TM) composite resin adhesive. Specimens were subjected to thermocycling and then to shear debonding forces on an Instron machine. Removal of the porcelain glaze, or use of hydrofluoric acid, prior to bonding were found to be unnecessary to secure the target bond strength. Hydrofluoric acid application was associated with increased porcelain surface damage. Thermocycling caused a significant reduction in shear bond strength to porcelain (P < 0*001). The best regime for orthodontic bonding to feldspathic porcelain was to apply phosphoric acid for 60 seconds, and prime with silane prior to bonding. Usually the porcelain surfaces could be repolished. Refereed Paper</p>","PeriodicalId":75621,"journal":{"name":"British journal of orthodontics","volume":"26 4","pages":"285-90"},"PeriodicalIF":0.0000,"publicationDate":"1999-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://sci-hub-pdf.com/10.1093/ortho/26.4.285","citationCount":"0","resultStr":"{\"title\":\"Factors affecting the shear bond strength of orthodontic brackets to porcelain.\",\"authors\":\"B M Bourke,&nbsp;W P Rock\",\"doi\":\"10.1093/ortho/26.4.285\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>The aim of this investigation was to establish a regime for orthodontic bonding to feldspathic porcelain, which ensures adequate bond strength (6-8 MPa) with minimal damage on debond and consisted of an ex vivo investigation measuring the effects of porcelain surface preparation and thermocycling on shear bond strength of orthodontic brackets. One-hundred-and-twenty feldspathic porcelain bonded crown surfaces were divided into 12 equally-sized groups to assess the effects of: (1) glaze removal, (2) application of hydrofluoric acid, phosphoric acid, or omission of acid treatment, and (3) silane priming upon the bond strength of premolar brackets bonded with Right-on (TM) composite resin adhesive. Specimens were subjected to thermocycling and then to shear debonding forces on an Instron machine. Removal of the porcelain glaze, or use of hydrofluoric acid, prior to bonding were found to be unnecessary to secure the target bond strength. Hydrofluoric acid application was associated with increased porcelain surface damage. Thermocycling caused a significant reduction in shear bond strength to porcelain (P < 0*001). The best regime for orthodontic bonding to feldspathic porcelain was to apply phosphoric acid for 60 seconds, and prime with silane prior to bonding. Usually the porcelain surfaces could be repolished. Refereed Paper</p>\",\"PeriodicalId\":75621,\"journal\":{\"name\":\"British journal of orthodontics\",\"volume\":\"26 4\",\"pages\":\"285-90\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1999-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://sci-hub-pdf.com/10.1093/ortho/26.4.285\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"British journal of orthodontics\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1093/ortho/26.4.285\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"British journal of orthodontics","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1093/ortho/26.4.285","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

本研究的目的是建立一种正畸与长石瓷结合的机制,以确保足够的结合强度(6-8 MPa),同时对脱落的损伤最小,并包括一个离体研究,测量瓷表面制备和热循环对正畸托槽剪切结合强度的影响。120个长石瓷粘接的牙冠表面被分成12个大小相等的组来评估:(1)去除釉料,(2)使用氢氟酸、磷酸或不使用酸处理,以及(3)硅烷对右置(TM)复合树脂胶粘剂粘接前磨牙托的粘接强度的影响。试样进行热循环,然后在Instron机器上进行剪切脱粘。去除瓷釉,或使用氢氟酸,在粘合之前被发现是不必要的,以确保目标粘结强度。氢氟酸应用与瓷表面损伤增加有关。热循环导致瓷的剪切结合强度显著降低(P < 0*001)。长石瓷正畸粘接的最佳方法是应用磷酸60秒,并在粘接前用硅烷进行初始处理。通常瓷器表面可以重新抛光。执法纸
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Factors affecting the shear bond strength of orthodontic brackets to porcelain.

The aim of this investigation was to establish a regime for orthodontic bonding to feldspathic porcelain, which ensures adequate bond strength (6-8 MPa) with minimal damage on debond and consisted of an ex vivo investigation measuring the effects of porcelain surface preparation and thermocycling on shear bond strength of orthodontic brackets. One-hundred-and-twenty feldspathic porcelain bonded crown surfaces were divided into 12 equally-sized groups to assess the effects of: (1) glaze removal, (2) application of hydrofluoric acid, phosphoric acid, or omission of acid treatment, and (3) silane priming upon the bond strength of premolar brackets bonded with Right-on (TM) composite resin adhesive. Specimens were subjected to thermocycling and then to shear debonding forces on an Instron machine. Removal of the porcelain glaze, or use of hydrofluoric acid, prior to bonding were found to be unnecessary to secure the target bond strength. Hydrofluoric acid application was associated with increased porcelain surface damage. Thermocycling caused a significant reduction in shear bond strength to porcelain (P < 0*001). The best regime for orthodontic bonding to feldspathic porcelain was to apply phosphoric acid for 60 seconds, and prime with silane prior to bonding. Usually the porcelain surfaces could be repolished. Refereed Paper

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信