{"title":"柔瓷镶嵌瓷的烧结缺陷。","authors":"B O Olorunfemi","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>The development of processing flaws within Flexoceram inlay porcelain prior to fracture strength testing was assessed qualitatively. The firing procedure recommended by the manufacturer was used except for the end-firing temperature which was varied. Sintering for 10 minutes produced less porous samples which were better than the manufacturer's recommended time of 9 minutes.</p>","PeriodicalId":76983,"journal":{"name":"African dental journal : official publication of the Federation of African Dental Associations = Journal dentaire africain","volume":"10 ","pages":"9-11"},"PeriodicalIF":0.0000,"publicationDate":"1996-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Sintering flaws in Flexoceram inlay porcelain.\",\"authors\":\"B O Olorunfemi\",\"doi\":\"\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>The development of processing flaws within Flexoceram inlay porcelain prior to fracture strength testing was assessed qualitatively. The firing procedure recommended by the manufacturer was used except for the end-firing temperature which was varied. Sintering for 10 minutes produced less porous samples which were better than the manufacturer's recommended time of 9 minutes.</p>\",\"PeriodicalId\":76983,\"journal\":{\"name\":\"African dental journal : official publication of the Federation of African Dental Associations = Journal dentaire africain\",\"volume\":\"10 \",\"pages\":\"9-11\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1996-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"African dental journal : official publication of the Federation of African Dental Associations = Journal dentaire africain\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"African dental journal : official publication of the Federation of African Dental Associations = Journal dentaire africain","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
The development of processing flaws within Flexoceram inlay porcelain prior to fracture strength testing was assessed qualitatively. The firing procedure recommended by the manufacturer was used except for the end-firing temperature which was varied. Sintering for 10 minutes produced less porous samples which were better than the manufacturer's recommended time of 9 minutes.