{"title":"低熔点Ni-Cu-Mn合金的腐蚀行为及热处理。","authors":"K Wakasa, M Yamaki","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>The appropriate procedure to improve corrosive property of B-grain in Ni-Cu-Mn casting alloy was to do the heat treatment at 350 degrees C for 6 hrs, because heavy corrosive behaviour was observed for only B-grain in dendritic A-grain, disk-like B-grain and very large C-grain. Then, new grain with corrosion-resistance appeared at previous location of B-grain.</p>","PeriodicalId":76541,"journal":{"name":"Shika rikogaku zasshi. Journal of the Japan Society for Dental Apparatus and Materials","volume":"22 60","pages":"295-8"},"PeriodicalIF":0.0000,"publicationDate":"1981-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Corrosion behaviour and heat treatment in low-melting Ni-Cu-Mn alloy.\",\"authors\":\"K Wakasa, M Yamaki\",\"doi\":\"\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>The appropriate procedure to improve corrosive property of B-grain in Ni-Cu-Mn casting alloy was to do the heat treatment at 350 degrees C for 6 hrs, because heavy corrosive behaviour was observed for only B-grain in dendritic A-grain, disk-like B-grain and very large C-grain. Then, new grain with corrosion-resistance appeared at previous location of B-grain.</p>\",\"PeriodicalId\":76541,\"journal\":{\"name\":\"Shika rikogaku zasshi. Journal of the Japan Society for Dental Apparatus and Materials\",\"volume\":\"22 60\",\"pages\":\"295-8\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1981-10-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Shika rikogaku zasshi. Journal of the Japan Society for Dental Apparatus and Materials\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Shika rikogaku zasshi. Journal of the Japan Society for Dental Apparatus and Materials","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Corrosion behaviour and heat treatment in low-melting Ni-Cu-Mn alloy.
The appropriate procedure to improve corrosive property of B-grain in Ni-Cu-Mn casting alloy was to do the heat treatment at 350 degrees C for 6 hrs, because heavy corrosive behaviour was observed for only B-grain in dendritic A-grain, disk-like B-grain and very large C-grain. Then, new grain with corrosion-resistance appeared at previous location of B-grain.