{"title":"将二氧化硅渗入作为克服氧化锆降解的一种策略","authors":"Najm M. Alfrisany,&nbsp;Eszter Somogyi-Ganss,&nbsp;Laura E Tam,&nbsp;Benjamin D. Hatton,&nbsp;Rana N. S. Sodhi,&nbsp;Ling Yin,&nbsp;Grace M. De Souza","doi":"10.1186/s40712-024-00180-w","DOIUrl":null,"url":null,"abstract":"<div><p>The excellent clinical performance of yttria-partially stabilized zirconias (Y-SZs) makes them promising materials for indirect restorations. However, the Y-SZ phase stability is a concern, and infiltrating Y-SZs with a silica nanofilm may delay their degradation processes. In this study, we analyzed stabilities of silica-infiltrated zirconia surfaces after exposure to artificial aging (AA).</p><p>Four zirconia materials with different translucencies (<i>n</i> = 40) were used, including low translucency 3 mol% Y-SZ (3Y-LT, Ceramill ZI, Amann Girrbach); high translucency 4 mol% Y-SZ (4Y-HT, Ceramill Zolid); and two high translucency 5 mol% Y-SZs (5Y-HT, Lava Esthetic, 3M and 5Y-SHT, Ceramill Zolid, FX white). Sintered specimens were exposed to 40 cycles of silica (SiO<sub>2</sub>) through room temperature atomic layer deposition (RT-ALD) using tetramethoxysilane (TMOS) and ammonium hydroxide (NH<sub>4</sub>OH). AA was applied for 15 h in an autoclave (134°C, 2 bar pressure). Stabilities of zirconia-silica surfaces were characterized in terms of hardness and Young's modulus using nanoindentation techniques and crystalline contents using x-ray diffraction (XRD) analyses. Silica deposition was also characterized by X-ray photoelectron spectroscopy (XPS).</p><p>There was a significant effect of the interaction of materials and surface treatments on the hardness and Young's modulus values of zirconia-silica surfaces (<i>p</i> &lt; 0.001). Silica deposition on zirconia surfaces improved the material resistance to degradation by AA.</p></div>","PeriodicalId":592,"journal":{"name":"International Journal of Mechanical and Materials Engineering","volume":"19 1","pages":""},"PeriodicalIF":3.4000,"publicationDate":"2024-09-14","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://jmsg.springeropen.com/counter/pdf/10.1186/s40712-024-00180-w","citationCount":"0","resultStr":"{\"title\":\"Silica infiltration as a strategy to overcome zirconia degradation\",\"authors\":\"Najm M. Alfrisany,&nbsp;Eszter Somogyi-Ganss,&nbsp;Laura E Tam,&nbsp;Benjamin D. Hatton,&nbsp;Rana N. S. Sodhi,&nbsp;Ling Yin,&nbsp;Grace M. De Souza\",\"doi\":\"10.1186/s40712-024-00180-w\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>The excellent clinical performance of yttria-partially stabilized zirconias (Y-SZs) makes them promising materials for indirect restorations. However, the Y-SZ phase stability is a concern, and infiltrating Y-SZs with a silica nanofilm may delay their degradation processes. In this study, we analyzed stabilities of silica-infiltrated zirconia surfaces after exposure to artificial aging (AA).</p><p>Four zirconia materials with different translucencies (<i>n</i> = 40) were used, including low translucency 3 mol% Y-SZ (3Y-LT, Ceramill ZI, Amann Girrbach); high translucency 4 mol% Y-SZ (4Y-HT, Ceramill Zolid); and two high translucency 5 mol% Y-SZs (5Y-HT, Lava Esthetic, 3M and 5Y-SHT, Ceramill Zolid, FX white). Sintered specimens were exposed to 40 cycles of silica (SiO<sub>2</sub>) through room temperature atomic layer deposition (RT-ALD) using tetramethoxysilane (TMOS) and ammonium hydroxide (NH<sub>4</sub>OH). AA was applied for 15 h in an autoclave (134°C, 2 bar pressure). Stabilities of zirconia-silica surfaces were characterized in terms of hardness and Young's modulus using nanoindentation techniques and crystalline contents using x-ray diffraction (XRD) analyses. Silica deposition was also characterized by X-ray photoelectron spectroscopy (XPS).</p><p>There was a significant effect of the interaction of materials and surface treatments on the hardness and Young's modulus values of zirconia-silica surfaces (<i>p</i> &lt; 0.001). Silica deposition on zirconia surfaces improved the material resistance to degradation by AA.</p></div>\",\"PeriodicalId\":592,\"journal\":{\"name\":\"International Journal of Mechanical and Materials Engineering\",\"volume\":\"19 1\",\"pages\":\"\"},\"PeriodicalIF\":3.4000,\"publicationDate\":\"2024-09-14\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://jmsg.springeropen.com/counter/pdf/10.1186/s40712-024-00180-w\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"International Journal of Mechanical and Materials Engineering\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://link.springer.com/article/10.1186/s40712-024-00180-w\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"MATERIALS SCIENCE, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Mechanical and Materials Engineering","FirstCategoryId":"1085","ListUrlMain":"https://link.springer.com/article/10.1186/s40712-024-00180-w","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

摘要

钇部分稳定锆石(Y-SZ)具有出色的临床表现,是一种很有前途的间接修复材料。然而,Y-SZ 相的稳定性是一个令人担忧的问题,用二氧化硅纳米薄膜渗入 Y-SZ 可能会延缓其降解过程。在这项研究中,我们分析了二氧化硅浸润氧化锆表面暴露于人工老化(AA)后的稳定性。我们使用了四种不同透光度的氧化锆材料(n = 40),包括低透光度 3 mol% Y-SZ(3Y-LT,Ceramill ZI,Amann Girrbach);高透光度 4 mol% Y-SZ(4Y-HT,Ceramill Zolid);以及两种高透光度 5 mol% Y-SZ(5Y-HT,Lava Esthetic,3M 和 5Y-SHT,Ceramill Zolid,FX white)。通过使用四甲氧基硅烷 (TMOS) 和氢氧化铵 (NH4OH) 进行室温原子层沉积 (RT-ALD),烧结试样暴露于二氧化硅 (SiO2) 40 个周期。AA 在高压釜(134°C,2 巴压力)中应用 15 小时。氧化锆-二氧化硅表面的稳定性通过纳米压痕技术的硬度和杨氏模量以及 X 射线衍射 (XRD) 分析的结晶含量来表征。材料和表面处理的相互作用对氧化锆-二氧化硅表面的硬度和杨氏模量值有显著影响(p < 0.001)。氧化锆表面的二氧化硅沉积提高了材料抗 AA 降解的能力。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Silica infiltration as a strategy to overcome zirconia degradation

The excellent clinical performance of yttria-partially stabilized zirconias (Y-SZs) makes them promising materials for indirect restorations. However, the Y-SZ phase stability is a concern, and infiltrating Y-SZs with a silica nanofilm may delay their degradation processes. In this study, we analyzed stabilities of silica-infiltrated zirconia surfaces after exposure to artificial aging (AA).

Four zirconia materials with different translucencies (n = 40) were used, including low translucency 3 mol% Y-SZ (3Y-LT, Ceramill ZI, Amann Girrbach); high translucency 4 mol% Y-SZ (4Y-HT, Ceramill Zolid); and two high translucency 5 mol% Y-SZs (5Y-HT, Lava Esthetic, 3M and 5Y-SHT, Ceramill Zolid, FX white). Sintered specimens were exposed to 40 cycles of silica (SiO2) through room temperature atomic layer deposition (RT-ALD) using tetramethoxysilane (TMOS) and ammonium hydroxide (NH4OH). AA was applied for 15 h in an autoclave (134°C, 2 bar pressure). Stabilities of zirconia-silica surfaces were characterized in terms of hardness and Young's modulus using nanoindentation techniques and crystalline contents using x-ray diffraction (XRD) analyses. Silica deposition was also characterized by X-ray photoelectron spectroscopy (XPS).

There was a significant effect of the interaction of materials and surface treatments on the hardness and Young's modulus values of zirconia-silica surfaces (p < 0.001). Silica deposition on zirconia surfaces improved the material resistance to degradation by AA.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
8.60
自引率
0.00%
发文量
1
审稿时长
13 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信