LPBF 工艺参数对 Cu-Cr-Zr 合金磨损特性的相关性分析

IF 2 3区 材料科学 Q2 ENGINEERING, MECHANICAL
M Saravana Kumar, N Jeyaprakash and Che-Hua Yang
{"title":"LPBF 工艺参数对 Cu-Cr-Zr 合金磨损特性的相关性分析","authors":"M Saravana Kumar, N Jeyaprakash and Che-Hua Yang","doi":"10.1088/2051-672x/ad76c2","DOIUrl":null,"url":null,"abstract":"Copper alloy bearings, gears, and fasteners have a significant impact on industrial sectors. However, due to the defect formation and void generation during the manufacturing of copper alloy parts using (Laser Powder Bed Fusion) LPBF technique, the wear resistance of the copper alloy was significantly affected. Hence, the prime novelty of the current research is enhancing wear resistance by analyzing the interaction of combined LPBF parameters. In order to decrease cavity forms and reduce the wear rate of the printed Cu alloy components, the important LPBF process parameters such as Scan Velocity (SV) of 550, 750, and 950 mm s−1, Laser Power (LP) of 460, 540, and 620 W, and Re-melting Range (RR) of 5, 25, and 45% were selected and studied. The results of the experimental investigation were supported by the use of Grey Relation Analysis (GRA). A comparative study was conducted with five distinct parameter combinations to investigate the relative influence of each parameter on the relative density, wear rate and elastic modulus. The research findings verify that the application of optimal SV of 750 mm s−1 and RR of 45% with maximum LP of 460 W resulted in the maximum relative density of 99.91%, minimal wear rate of 0.52 × 10−5 mm3/Nm, and maximum elastic modulus of 140.22 GPa.","PeriodicalId":22028,"journal":{"name":"Surface Topography: Metrology and Properties","volume":"2012 1","pages":""},"PeriodicalIF":2.0000,"publicationDate":"2024-09-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Analysis of co-relation on LPBF process parameter on wear characteristics of Cu-Cr-Zr alloy\",\"authors\":\"M Saravana Kumar, N Jeyaprakash and Che-Hua Yang\",\"doi\":\"10.1088/2051-672x/ad76c2\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Copper alloy bearings, gears, and fasteners have a significant impact on industrial sectors. However, due to the defect formation and void generation during the manufacturing of copper alloy parts using (Laser Powder Bed Fusion) LPBF technique, the wear resistance of the copper alloy was significantly affected. Hence, the prime novelty of the current research is enhancing wear resistance by analyzing the interaction of combined LPBF parameters. In order to decrease cavity forms and reduce the wear rate of the printed Cu alloy components, the important LPBF process parameters such as Scan Velocity (SV) of 550, 750, and 950 mm s−1, Laser Power (LP) of 460, 540, and 620 W, and Re-melting Range (RR) of 5, 25, and 45% were selected and studied. The results of the experimental investigation were supported by the use of Grey Relation Analysis (GRA). A comparative study was conducted with five distinct parameter combinations to investigate the relative influence of each parameter on the relative density, wear rate and elastic modulus. The research findings verify that the application of optimal SV of 750 mm s−1 and RR of 45% with maximum LP of 460 W resulted in the maximum relative density of 99.91%, minimal wear rate of 0.52 × 10−5 mm3/Nm, and maximum elastic modulus of 140.22 GPa.\",\"PeriodicalId\":22028,\"journal\":{\"name\":\"Surface Topography: Metrology and Properties\",\"volume\":\"2012 1\",\"pages\":\"\"},\"PeriodicalIF\":2.0000,\"publicationDate\":\"2024-09-10\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Surface Topography: Metrology and Properties\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.1088/2051-672x/ad76c2\",\"RegionNum\":3,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"ENGINEERING, MECHANICAL\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Surface Topography: Metrology and Properties","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1088/2051-672x/ad76c2","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"ENGINEERING, MECHANICAL","Score":null,"Total":0}
引用次数: 0

摘要

铜合金轴承、齿轮和紧固件对工业领域有着重要影响。然而,在使用(激光粉末床熔融)LPBF 技术制造铜合金零件的过程中,由于缺陷的形成和空隙的产生,铜合金的耐磨性受到了严重影响。因此,本研究的主要创新点是通过分析 LPBF 组合参数的相互作用来提高耐磨性。为了减少印刷铜合金部件的空腔形状并降低磨损率,研究人员选择并研究了重要的 LPBF 工艺参数,如扫描速度(SV)为 550、750 和 950 mm s-1,激光功率(LP)为 460、540 和 620 W,再熔范围(RR)为 5、25 和 45%。实验调查的结果得到了灰色关系分析法(GRA)的支持。通过五种不同的参数组合进行了对比研究,以探究每种参数对相对密度、磨损率和弹性模量的相对影响。研究结果证实,采用最佳 SV 值 750 mm s-1 和 RR 值 45%,最大 LP 值 460 W 时,相对密度最大为 99.91%,磨损率最小为 0.52 × 10-5 mm3/Nm,弹性模量最大为 140.22 GPa。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Analysis of co-relation on LPBF process parameter on wear characteristics of Cu-Cr-Zr alloy
Copper alloy bearings, gears, and fasteners have a significant impact on industrial sectors. However, due to the defect formation and void generation during the manufacturing of copper alloy parts using (Laser Powder Bed Fusion) LPBF technique, the wear resistance of the copper alloy was significantly affected. Hence, the prime novelty of the current research is enhancing wear resistance by analyzing the interaction of combined LPBF parameters. In order to decrease cavity forms and reduce the wear rate of the printed Cu alloy components, the important LPBF process parameters such as Scan Velocity (SV) of 550, 750, and 950 mm s−1, Laser Power (LP) of 460, 540, and 620 W, and Re-melting Range (RR) of 5, 25, and 45% were selected and studied. The results of the experimental investigation were supported by the use of Grey Relation Analysis (GRA). A comparative study was conducted with five distinct parameter combinations to investigate the relative influence of each parameter on the relative density, wear rate and elastic modulus. The research findings verify that the application of optimal SV of 750 mm s−1 and RR of 45% with maximum LP of 460 W resulted in the maximum relative density of 99.91%, minimal wear rate of 0.52 × 10−5 mm3/Nm, and maximum elastic modulus of 140.22 GPa.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Surface Topography: Metrology and Properties
Surface Topography: Metrology and Properties Materials Science-Materials Chemistry
CiteScore
4.10
自引率
22.20%
发文量
183
期刊介绍: An international forum for academics, industrialists and engineers to publish the latest research in surface topography measurement and characterisation, instrumentation development and the properties of surfaces.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信