三维 Cu3N 纳米线/铜泡沫复合宿主可实现高容量和长储能锂电池

IF 7.2 2区 材料科学 Q1 MATERIALS SCIENCE, MULTIDISCIPLINARY
Jialu Liu, Haijun Tian, Yingke Zhou, Enmin Xu, Ping Li, Xiaohui Tian, Zhongzhi Yuan
{"title":"三维 Cu3N 纳米线/铜泡沫复合宿主可实现高容量和长储能锂电池","authors":"Jialu Liu, Haijun Tian, Yingke Zhou, Enmin Xu, Ping Li, Xiaohui Tian, Zhongzhi Yuan","doi":"10.1016/j.apmt.2024.102378","DOIUrl":null,"url":null,"abstract":"Lithium batteries are widely used in electronic and medical devices for the advantages of high energy/power densities and low self-discharge. However, the active lithium metal anode can react with electrolyte to form unstable solid electrolyte interface (SEI) and affect the rate performance and stability of lithium batteries. In this work, we design a 3D Cu foam (CF) based copper nitride nanowire (CuN NW) array, and further construct stable 3D composite Li anode by molten lithium metal infusion method. CuN NWs can improve the lithiophilicity and ionic conductivity, and provide high specific surface area, uniform local current density and abundant diffusion channels for lithium-ion flux. The designed 3D CuN NW/Cu foam electrode achieves uniform lithium deposition, excellent discharge performance and stability under high temperature and long-term storage conditions. The Li@CuN NW/CF-CF battery exhibits excellent discharge specific capacity of 1080 mAh g (0.1 C) and remarkable rate capacity of 546 mAh g (8 C). After 60 days of storage at room temperature and 55 °C, the battery also demonstrates excellent storage performance of 874 and 627 mAh g. This work provides a facile and effective strategy for designing stable composite Li anode with a LiN-rich SEI for high-performance lithium batteries.","PeriodicalId":8066,"journal":{"name":"Applied Materials Today","volume":"3 1","pages":""},"PeriodicalIF":7.2000,"publicationDate":"2024-08-07","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"3D Cu3N nanowire/Cu foam composite host enables high-capacity and long-storage lithium battery\",\"authors\":\"Jialu Liu, Haijun Tian, Yingke Zhou, Enmin Xu, Ping Li, Xiaohui Tian, Zhongzhi Yuan\",\"doi\":\"10.1016/j.apmt.2024.102378\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Lithium batteries are widely used in electronic and medical devices for the advantages of high energy/power densities and low self-discharge. However, the active lithium metal anode can react with electrolyte to form unstable solid electrolyte interface (SEI) and affect the rate performance and stability of lithium batteries. In this work, we design a 3D Cu foam (CF) based copper nitride nanowire (CuN NW) array, and further construct stable 3D composite Li anode by molten lithium metal infusion method. CuN NWs can improve the lithiophilicity and ionic conductivity, and provide high specific surface area, uniform local current density and abundant diffusion channels for lithium-ion flux. The designed 3D CuN NW/Cu foam electrode achieves uniform lithium deposition, excellent discharge performance and stability under high temperature and long-term storage conditions. The Li@CuN NW/CF-CF battery exhibits excellent discharge specific capacity of 1080 mAh g (0.1 C) and remarkable rate capacity of 546 mAh g (8 C). After 60 days of storage at room temperature and 55 °C, the battery also demonstrates excellent storage performance of 874 and 627 mAh g. This work provides a facile and effective strategy for designing stable composite Li anode with a LiN-rich SEI for high-performance lithium batteries.\",\"PeriodicalId\":8066,\"journal\":{\"name\":\"Applied Materials Today\",\"volume\":\"3 1\",\"pages\":\"\"},\"PeriodicalIF\":7.2000,\"publicationDate\":\"2024-08-07\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Applied Materials Today\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.1016/j.apmt.2024.102378\",\"RegionNum\":2,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"MATERIALS SCIENCE, MULTIDISCIPLINARY\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Applied Materials Today","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1016/j.apmt.2024.102378","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

摘要

锂电池具有高能量/功率密度和低自放电的优点,被广泛应用于电子和医疗设备中。然而,活性锂金属阳极会与电解质发生反应,形成不稳定的固体电解质界面(SEI),影响锂电池的速率性能和稳定性。在这项研究中,我们设计了一种基于三维铜泡沫(CF)的氮化铜纳米线(CuN NW)阵列,并进一步通过熔融锂金属注入法构建了稳定的三维复合锂负极。氮化铜纳米线能提高锂离子的亲锂性和离子导电性,并为锂离子通量提供高比表面积、均匀的局部电流密度和丰富的扩散通道。所设计的三维 CuN NW/Cu 泡沫电极可实现均匀的锂沉积、优异的放电性能以及在高温和长期储存条件下的稳定性。Li@CuN NW/CF-CF 电池的放电比容量为 1080 mAh g (0.1 C),速率容量为 546 mAh g (8 C)。在室温和 55 °C条件下存储 60 天后,该电池还显示出 874 mAh g 和 627 mAh g 的优异存储性能。这项工作为设计稳定的复合锂负极和高性能锂电池的富含 LiN 的 SEI 提供了一种简便有效的策略。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
3D Cu3N nanowire/Cu foam composite host enables high-capacity and long-storage lithium battery
Lithium batteries are widely used in electronic and medical devices for the advantages of high energy/power densities and low self-discharge. However, the active lithium metal anode can react with electrolyte to form unstable solid electrolyte interface (SEI) and affect the rate performance and stability of lithium batteries. In this work, we design a 3D Cu foam (CF) based copper nitride nanowire (CuN NW) array, and further construct stable 3D composite Li anode by molten lithium metal infusion method. CuN NWs can improve the lithiophilicity and ionic conductivity, and provide high specific surface area, uniform local current density and abundant diffusion channels for lithium-ion flux. The designed 3D CuN NW/Cu foam electrode achieves uniform lithium deposition, excellent discharge performance and stability under high temperature and long-term storage conditions. The Li@CuN NW/CF-CF battery exhibits excellent discharge specific capacity of 1080 mAh g (0.1 C) and remarkable rate capacity of 546 mAh g (8 C). After 60 days of storage at room temperature and 55 °C, the battery also demonstrates excellent storage performance of 874 and 627 mAh g. This work provides a facile and effective strategy for designing stable composite Li anode with a LiN-rich SEI for high-performance lithium batteries.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Applied Materials Today
Applied Materials Today Materials Science-General Materials Science
CiteScore
14.90
自引率
3.60%
发文量
393
审稿时长
26 days
期刊介绍: Journal Name: Applied Materials Today Focus: Multi-disciplinary, rapid-publication journal Focused on cutting-edge applications of novel materials Overview: New materials discoveries have led to exciting fundamental breakthroughs. Materials research is now moving towards the translation of these scientific properties and principles.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信