{"title":"600 至 750 °C 等温退火对 SAF 2205 双相不锈钢降解的影响","authors":"J. Burja, B. Žužek, B. Šetina Batič","doi":"10.3390/cmd5030014","DOIUrl":null,"url":null,"abstract":"We studied the effect of isothermal annealing (600–750 °C, 1 to 1000 min) on the microstructure and mechanical properties of SAF 2205 duplex stainless steel. Impact toughness was found to be significantly more affected than hardness by annealing. Annealing at 750 °C for 1000 min resulted in a more than 90% decrease in impact toughness, while hardness only increased by 25%. Tensile strength increased up to 100 MPa, but elongation decreased by more than 50% under the same conditions. Sigma phase formation was minimal at lower temperatures (650 °C and below) but increased significantly at higher temperatures. At 750 °C and 1000 min of annealing, the ferrite content dropped from 50% to 16%. These findings suggest that annealing temperature and time need to be carefully controlled to avoid a reduction in impact toughness and ductility caused by sigma phase precipitation. The harmful effect of sigma phase precipitation on mechanical properties was directly shown.","PeriodicalId":10693,"journal":{"name":"Corrosion and Materials Degradation","volume":"32 3","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-07-12","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Influence of Isothermal Annealing in the 600 to 750 °C Range on the Degradation of SAF 2205 Duplex Stainless Steel\",\"authors\":\"J. Burja, B. Žužek, B. Šetina Batič\",\"doi\":\"10.3390/cmd5030014\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"We studied the effect of isothermal annealing (600–750 °C, 1 to 1000 min) on the microstructure and mechanical properties of SAF 2205 duplex stainless steel. Impact toughness was found to be significantly more affected than hardness by annealing. Annealing at 750 °C for 1000 min resulted in a more than 90% decrease in impact toughness, while hardness only increased by 25%. Tensile strength increased up to 100 MPa, but elongation decreased by more than 50% under the same conditions. Sigma phase formation was minimal at lower temperatures (650 °C and below) but increased significantly at higher temperatures. At 750 °C and 1000 min of annealing, the ferrite content dropped from 50% to 16%. These findings suggest that annealing temperature and time need to be carefully controlled to avoid a reduction in impact toughness and ductility caused by sigma phase precipitation. The harmful effect of sigma phase precipitation on mechanical properties was directly shown.\",\"PeriodicalId\":10693,\"journal\":{\"name\":\"Corrosion and Materials Degradation\",\"volume\":\"32 3\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2024-07-12\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Corrosion and Materials Degradation\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.3390/cmd5030014\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Corrosion and Materials Degradation","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3390/cmd5030014","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

我们研究了等温退火(600-750 °C,1 至 1000 分钟)对 SAF 2205 双相不锈钢微观结构和机械性能的影响。研究发现,退火对冲击韧性的影响明显大于对硬度的影响。750 °C 退火 1000 分钟导致冲击韧性下降超过 90%,而硬度仅增加 25%。在相同条件下,拉伸强度增加到 100 兆帕,但伸长率下降了 50%以上。在较低温度(650 °C及以下)下,西格玛相的形成极少,但在较高温度下,西格玛相的形成显著增加。在 750 °C 和 1000 分钟退火条件下,铁素体含量从 50% 降至 16%。这些发现表明,需要仔细控制退火温度和时间,以避免σ相析出导致冲击韧性和延展性降低。直接显示了σ相析出对机械性能的有害影响。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Influence of Isothermal Annealing in the 600 to 750 °C Range on the Degradation of SAF 2205 Duplex Stainless Steel
We studied the effect of isothermal annealing (600–750 °C, 1 to 1000 min) on the microstructure and mechanical properties of SAF 2205 duplex stainless steel. Impact toughness was found to be significantly more affected than hardness by annealing. Annealing at 750 °C for 1000 min resulted in a more than 90% decrease in impact toughness, while hardness only increased by 25%. Tensile strength increased up to 100 MPa, but elongation decreased by more than 50% under the same conditions. Sigma phase formation was minimal at lower temperatures (650 °C and below) but increased significantly at higher temperatures. At 750 °C and 1000 min of annealing, the ferrite content dropped from 50% to 16%. These findings suggest that annealing temperature and time need to be carefully controlled to avoid a reduction in impact toughness and ductility caused by sigma phase precipitation. The harmful effect of sigma phase precipitation on mechanical properties was directly shown.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
CiteScore
4.50
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信