Tao-tao Li, Hong-de Ding, Rui-feng Li, Kai Qi, Zhen-guang Liu, Xiao-qiang Zhang, Yue Zhao, Lei Qiao
{"title":"无针搅拌摩擦点焊镁/钢搭接接头的孔抑制机理","authors":"Tao-tao Li, Hong-de Ding, Rui-feng Li, Kai Qi, Zhen-guang Liu, Xiao-qiang Zhang, Yue Zhao, Lei Qiao","doi":"10.1007/s42243-024-01263-w","DOIUrl":null,"url":null,"abstract":"<p>Pinless friction stir spot welding (P-FSSW) was performed to manufacture Mg/steel lap joints. Orthogonal tests for P-FSSW of Mg/steel were investigated, and the main factors affecting the properties of Mg/steel lap joints were derived. The shear force of the Mg/steel lap joints gradually increased and then decreased as the welding time increased. Maximum shear force was 5.3 kN. Fe–Al intermetallic compound (IMC) was formed at the Mg/steel interface near the steel side, and Mg–Al IMCs were formed at the Mg/steel interface near the Mg alloy side. Mg/steel lap joint was transformed from an initial solid-state welding to fusion-brazing welding as the welding time increased. No hole defects were formed in Mg/steel solid-state welding joints, whereas hole defects appeared in Mg/steel fusion-brazing welding joints. The temperature field of Mg/steel lap joints was simulated to analyze hole defects generated during the welding process. Hole defects can be eliminated by changing the spindle deflection angle, and the shear force decreased. Excessive spindle deflection can also lead to failure to form a stable joint. Hole defects were removed because the spindle deflection angle reduced the interfacial reaction temperature, and a solid-state welding joint was formed, which resulted in an absence of fusion-brazing welding hole formation.</p>","PeriodicalId":16151,"journal":{"name":"Journal of Iron and Steel Research International","volume":null,"pages":null},"PeriodicalIF":2.5000,"publicationDate":"2024-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Hole inhibition mechanisms of Mg/steel lap joint by pinless friction stir spot welding\",\"authors\":\"Tao-tao Li, Hong-de Ding, Rui-feng Li, Kai Qi, Zhen-guang Liu, Xiao-qiang Zhang, Yue Zhao, Lei Qiao\",\"doi\":\"10.1007/s42243-024-01263-w\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>Pinless friction stir spot welding (P-FSSW) was performed to manufacture Mg/steel lap joints. Orthogonal tests for P-FSSW of Mg/steel were investigated, and the main factors affecting the properties of Mg/steel lap joints were derived. The shear force of the Mg/steel lap joints gradually increased and then decreased as the welding time increased. Maximum shear force was 5.3 kN. Fe–Al intermetallic compound (IMC) was formed at the Mg/steel interface near the steel side, and Mg–Al IMCs were formed at the Mg/steel interface near the Mg alloy side. Mg/steel lap joint was transformed from an initial solid-state welding to fusion-brazing welding as the welding time increased. No hole defects were formed in Mg/steel solid-state welding joints, whereas hole defects appeared in Mg/steel fusion-brazing welding joints. The temperature field of Mg/steel lap joints was simulated to analyze hole defects generated during the welding process. Hole defects can be eliminated by changing the spindle deflection angle, and the shear force decreased. Excessive spindle deflection can also lead to failure to form a stable joint. Hole defects were removed because the spindle deflection angle reduced the interfacial reaction temperature, and a solid-state welding joint was formed, which resulted in an absence of fusion-brazing welding hole formation.</p>\",\"PeriodicalId\":16151,\"journal\":{\"name\":\"Journal of Iron and Steel Research International\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":2.5000,\"publicationDate\":\"2024-07-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Iron and Steel Research International\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.1007/s42243-024-01263-w\",\"RegionNum\":2,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Iron and Steel Research International","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1007/s42243-024-01263-w","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

无针刺搅拌摩擦点焊(P-FSSW)用于制造镁/钢搭接接头。研究了镁/钢 P-FSSW 的正交试验,并得出了影响镁/钢搭接接头性能的主要因素。随着焊接时间的延长,镁/钢搭接接头的剪切力逐渐增大,然后减小。最大剪切力为 5.3 kN。靠近钢侧的镁/钢界面上形成了铁-铝金属间化合物(IMC),靠近镁合金侧的镁/钢界面上形成了镁-铝金属间化合物。随着焊接时间的延长,镁/钢搭接接头从最初的固态焊接转变为熔钎焊。镁/钢固态焊接接头没有形成孔洞缺陷,而镁/钢熔融钎焊接头则出现了孔洞缺陷。通过模拟镁/钢搭接接头的温度场来分析焊接过程中产生的孔缺陷。通过改变主轴偏转角度可以消除孔洞缺陷,同时降低剪切力。主轴偏转角度过大也会导致无法形成稳定的接头。由于主轴偏转角度降低了界面反应温度,消除了孔缺陷,形成了固态焊接接头,从而避免了熔钎焊孔的形成。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

Hole inhibition mechanisms of Mg/steel lap joint by pinless friction stir spot welding

Hole inhibition mechanisms of Mg/steel lap joint by pinless friction stir spot welding

Pinless friction stir spot welding (P-FSSW) was performed to manufacture Mg/steel lap joints. Orthogonal tests for P-FSSW of Mg/steel were investigated, and the main factors affecting the properties of Mg/steel lap joints were derived. The shear force of the Mg/steel lap joints gradually increased and then decreased as the welding time increased. Maximum shear force was 5.3 kN. Fe–Al intermetallic compound (IMC) was formed at the Mg/steel interface near the steel side, and Mg–Al IMCs were formed at the Mg/steel interface near the Mg alloy side. Mg/steel lap joint was transformed from an initial solid-state welding to fusion-brazing welding as the welding time increased. No hole defects were formed in Mg/steel solid-state welding joints, whereas hole defects appeared in Mg/steel fusion-brazing welding joints. The temperature field of Mg/steel lap joints was simulated to analyze hole defects generated during the welding process. Hole defects can be eliminated by changing the spindle deflection angle, and the shear force decreased. Excessive spindle deflection can also lead to failure to form a stable joint. Hole defects were removed because the spindle deflection angle reduced the interfacial reaction temperature, and a solid-state welding joint was formed, which resulted in an absence of fusion-brazing welding hole formation.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
16.00%
发文量
161
审稿时长
2.8 months
期刊介绍: Publishes critically reviewed original research of archival significance Covers hydrometallurgy, pyrometallurgy, electrometallurgy, transport phenomena, process control, physical chemistry, solidification, mechanical working, solid state reactions, materials processing, and more Includes welding & joining, surface treatment, mathematical modeling, corrosion, wear and abrasion Journal of Iron and Steel Research International publishes original papers and occasional invited reviews on aspects of research and technology in the process metallurgy and metallic materials. Coverage emphasizes the relationships among the processing, structure and properties of metals, including advanced steel materials, superalloy, intermetallics, metallic functional materials, powder metallurgy, structural titanium alloy, composite steel materials, high entropy alloy, amorphous alloys, metallic nanomaterials, etc..
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信