直接和间接复合材料贴面老化后的断裂强度:体外研究

IF 0.5 Q4 DENTISTRY, ORAL SURGERY & MEDICINE
Aishwarya Menon, Sowmya Kumar, C. Hegde
{"title":"直接和间接复合材料贴面老化后的断裂强度:体外研究","authors":"Aishwarya Menon, Sowmya Kumar, C. Hegde","doi":"10.4103/jioh.jioh_169_23","DOIUrl":null,"url":null,"abstract":"Aim: The number of patients seeking veneers for minor changes in the color, shape, and size of their anterior teeth has increased. On the basis of this requirement, with the advances in physical and optical properties, composite resins have become viable materials to be used for veneers. There is a paucity of studies that highlight the use of composite resins for anterior esthetic rehabilitations. Hence, this study aimed to compare the fracture strengths of direct and indirect composite veneers. Materials and Methods: This study was conducted on a total of 56 maxillary central incisor samples, divided into two groups: direct composite (n = 28) and indirect composite (n = 28) veneers. Tooth preparations were done, and composite veneers were made via the two techniques. Thermocycling was carried out to age the restorations for half the samples from both groups. The fracture test was performed in a universal testing machine where the load was applied from the incisal direction at the veneer–tooth interface. Results: Direct composite veneers showed a mean fracture strength of 485 ± 147 N before and 438 ± 199 N after thermocycling. Indirect composite veneers showed a mean fracture strength of 409 ± 179 N before and 254 ± 135 N after thermocycling. The most common mode of failure for direct composite veneers was veneer chipping and fracture, whereas debonding was most frequently noted for indirect composite veneers. Statistical analysis used: Unpaired t test was used to study the fracture strengths among the two groups before and after thermocycling. The comparison of frequencies of a mode of failure was investigated using the chi-square test. Conclusions: The direct composite resin veneers showed superior fracture strength, both before and after thermocycling.","PeriodicalId":16138,"journal":{"name":"Journal of International Oral Health","volume":"53 1","pages":"469 - 475"},"PeriodicalIF":0.5000,"publicationDate":"2023-09-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Fracture strength of direct and indirect composite veneers after aging: An in vitro study\",\"authors\":\"Aishwarya Menon, Sowmya Kumar, C. Hegde\",\"doi\":\"10.4103/jioh.jioh_169_23\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Aim: The number of patients seeking veneers for minor changes in the color, shape, and size of their anterior teeth has increased. On the basis of this requirement, with the advances in physical and optical properties, composite resins have become viable materials to be used for veneers. There is a paucity of studies that highlight the use of composite resins for anterior esthetic rehabilitations. Hence, this study aimed to compare the fracture strengths of direct and indirect composite veneers. Materials and Methods: This study was conducted on a total of 56 maxillary central incisor samples, divided into two groups: direct composite (n = 28) and indirect composite (n = 28) veneers. Tooth preparations were done, and composite veneers were made via the two techniques. Thermocycling was carried out to age the restorations for half the samples from both groups. The fracture test was performed in a universal testing machine where the load was applied from the incisal direction at the veneer–tooth interface. Results: Direct composite veneers showed a mean fracture strength of 485 ± 147 N before and 438 ± 199 N after thermocycling. Indirect composite veneers showed a mean fracture strength of 409 ± 179 N before and 254 ± 135 N after thermocycling. The most common mode of failure for direct composite veneers was veneer chipping and fracture, whereas debonding was most frequently noted for indirect composite veneers. Statistical analysis used: Unpaired t test was used to study the fracture strengths among the two groups before and after thermocycling. The comparison of frequencies of a mode of failure was investigated using the chi-square test. Conclusions: The direct composite resin veneers showed superior fracture strength, both before and after thermocycling.\",\"PeriodicalId\":16138,\"journal\":{\"name\":\"Journal of International Oral Health\",\"volume\":\"53 1\",\"pages\":\"469 - 475\"},\"PeriodicalIF\":0.5000,\"publicationDate\":\"2023-09-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of International Oral Health\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.4103/jioh.jioh_169_23\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q4\",\"JCRName\":\"DENTISTRY, ORAL SURGERY & MEDICINE\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of International Oral Health","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4103/jioh.jioh_169_23","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0

摘要

目的:因前牙的颜色、形状和大小发生微小变化而寻求贴面治疗的患者人数有所增加。基于这一需求,随着物理和光学特性的进步,复合树脂已成为贴面的可行材料。关于复合树脂在前牙美学修复中的应用的研究很少。因此,本研究旨在比较直接和间接复合树脂贴面的断裂强度。材料和方法:本研究共使用了 56 个上颌中切牙样本,分为两组:直接复合树脂贴面(28 个)和间接复合树脂贴面(28 个)。对牙齿进行制备,并通过两种技术制作复合材料贴面。对两组中一半的修复体进行热循环老化。断裂测试在万能试验机中进行,载荷从贴面与牙齿界面的切缘方向施加。结果显示直接复合材料贴面的平均断裂强度在热循环前为 485 ± 147 N,热循环后为 438 ± 199 N。间接复合材料贴面在热循环前的平均断裂强度为 409 ± 179 N,热循环后为 254 ± 135 N。直接复合材料贴面最常见的失效模式是贴面崩裂和断裂,而间接复合材料贴面最常见的失效模式是脱粘。使用的统计分析:采用非配对 t 检验来研究热循环前后两组的断裂强度。采用卡方检验对失效模式的频率进行比较。得出结论:直接复合树脂贴面在热循环前后的断裂强度均优于直接复合树脂贴面。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Fracture strength of direct and indirect composite veneers after aging: An in vitro study
Aim: The number of patients seeking veneers for minor changes in the color, shape, and size of their anterior teeth has increased. On the basis of this requirement, with the advances in physical and optical properties, composite resins have become viable materials to be used for veneers. There is a paucity of studies that highlight the use of composite resins for anterior esthetic rehabilitations. Hence, this study aimed to compare the fracture strengths of direct and indirect composite veneers. Materials and Methods: This study was conducted on a total of 56 maxillary central incisor samples, divided into two groups: direct composite (n = 28) and indirect composite (n = 28) veneers. Tooth preparations were done, and composite veneers were made via the two techniques. Thermocycling was carried out to age the restorations for half the samples from both groups. The fracture test was performed in a universal testing machine where the load was applied from the incisal direction at the veneer–tooth interface. Results: Direct composite veneers showed a mean fracture strength of 485 ± 147 N before and 438 ± 199 N after thermocycling. Indirect composite veneers showed a mean fracture strength of 409 ± 179 N before and 254 ± 135 N after thermocycling. The most common mode of failure for direct composite veneers was veneer chipping and fracture, whereas debonding was most frequently noted for indirect composite veneers. Statistical analysis used: Unpaired t test was used to study the fracture strengths among the two groups before and after thermocycling. The comparison of frequencies of a mode of failure was investigated using the chi-square test. Conclusions: The direct composite resin veneers showed superior fracture strength, both before and after thermocycling.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Journal of International Oral Health
Journal of International Oral Health Dentistry-Dentistry (all)
CiteScore
1.00
自引率
14.30%
发文量
15
期刊介绍: It is a journal aimed for research, scientific facts and details covering all specialties of dentistry with a good determination for exploring and sharing the knowledge in the medical and dental fraternity. The scope is therefore huge covering almost all streams of dentistry - starting from original studies, systematic reviews, narrative reviews, very unique case reports. Our journal appreciates research articles pertaining with advancement of dentistry. Journal scope is not limited to these subjects and is more wider covering all specialities of dentistry follows: Preventive and Community Dentistry (Dental Public Health) Endodontics Oral and Maxillofacial Pathology Oral and Maxillofacial Radiology Oral and Maxillofacial Surgery (also called Oral Surgery) Orthodontics and Dentofacial Orthopaedics Periodontology (also called Periodontics) Pediatric Dentistry (also called Pedodontics) Prosthodontics (also called Prosthetic Dentistry) Oral Medicine Special Needs Dentistry (also called Special Care Dentistry) Oral Biology Forensic Odontology Geriatric Dentistry or Geriodontics Implantology Laser and Aesthetic Dentistry.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信