{"title":"用不同比例的钛粒子强化并经 ECAP 加工的 AZ91 镁合金的力学性能提升","authors":"Song-Jeng Huang, Yu-Quan Lee, Y. Tanoto","doi":"10.6000/1929-5995.2023.12.19","DOIUrl":null,"url":null,"abstract":"This study utilized AZ91 magnesium-aluminum alloy as the matrix for magnesium-based composites, reinforced with micron-sized titanium (Ti). Gravity casting and mechanical stirring were employed to fabricate specimens with 0 wt.%, 0.3 wt.%, and 0.5 wt.% Ti reinforcement. Heat-treated samples underwent Equal Channel Angular Pressing (ECAP), and microstructures were analyzed via SEM and XRD. The experimental results demonstrate that the addition of micron-sized titanium improves the yield strength, ultimate tensile strength, and hardness. The inclusion of 0.5 wt.% titanium powder resulted in a 17.5% increase in ultimate tensile strength and a 37% increase in yield strength. After secondary processing with ECAP, the ultimate tensile strength showed an additional 25% increase, while the yield strength increased by 13.5%. Vickers hardness test results reveal a significant 13.7% strength improvement with the addition of 0.5 wt.% titanium powder, and after ECAP secondary processing, there was a marginal additional increase of 0.8%.","PeriodicalId":16998,"journal":{"name":"Journal of Research Updates in Polymer Science","volume":"17 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-11-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Mechanical Properties Enhancement of AZ91 Magnesium Alloy Reinforced with Various Ratios of Titanium Particles and Processed by ECAP\",\"authors\":\"Song-Jeng Huang, Yu-Quan Lee, Y. Tanoto\",\"doi\":\"10.6000/1929-5995.2023.12.19\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"This study utilized AZ91 magnesium-aluminum alloy as the matrix for magnesium-based composites, reinforced with micron-sized titanium (Ti). Gravity casting and mechanical stirring were employed to fabricate specimens with 0 wt.%, 0.3 wt.%, and 0.5 wt.% Ti reinforcement. Heat-treated samples underwent Equal Channel Angular Pressing (ECAP), and microstructures were analyzed via SEM and XRD. The experimental results demonstrate that the addition of micron-sized titanium improves the yield strength, ultimate tensile strength, and hardness. The inclusion of 0.5 wt.% titanium powder resulted in a 17.5% increase in ultimate tensile strength and a 37% increase in yield strength. After secondary processing with ECAP, the ultimate tensile strength showed an additional 25% increase, while the yield strength increased by 13.5%. Vickers hardness test results reveal a significant 13.7% strength improvement with the addition of 0.5 wt.% titanium powder, and after ECAP secondary processing, there was a marginal additional increase of 0.8%.\",\"PeriodicalId\":16998,\"journal\":{\"name\":\"Journal of Research Updates in Polymer Science\",\"volume\":\"17 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-11-30\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Journal of Research Updates in Polymer Science\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.6000/1929-5995.2023.12.19\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Research Updates in Polymer Science","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.6000/1929-5995.2023.12.19","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Mechanical Properties Enhancement of AZ91 Magnesium Alloy Reinforced with Various Ratios of Titanium Particles and Processed by ECAP
This study utilized AZ91 magnesium-aluminum alloy as the matrix for magnesium-based composites, reinforced with micron-sized titanium (Ti). Gravity casting and mechanical stirring were employed to fabricate specimens with 0 wt.%, 0.3 wt.%, and 0.5 wt.% Ti reinforcement. Heat-treated samples underwent Equal Channel Angular Pressing (ECAP), and microstructures were analyzed via SEM and XRD. The experimental results demonstrate that the addition of micron-sized titanium improves the yield strength, ultimate tensile strength, and hardness. The inclusion of 0.5 wt.% titanium powder resulted in a 17.5% increase in ultimate tensile strength and a 37% increase in yield strength. After secondary processing with ECAP, the ultimate tensile strength showed an additional 25% increase, while the yield strength increased by 13.5%. Vickers hardness test results reveal a significant 13.7% strength improvement with the addition of 0.5 wt.% titanium powder, and after ECAP secondary processing, there was a marginal additional increase of 0.8%.