Februriyana Pirade, Kim Lompe, Javier Jimenez-Lamana, Sulalit Bandyopadhyay, Katharina Zürbes, Nesrine Bali, Dušan Materić, Jan Willem Foppen
{"title":"金标法对天然水中纳米塑料的定量是否合适?","authors":"Februriyana Pirade, Kim Lompe, Javier Jimenez-Lamana, Sulalit Bandyopadhyay, Katharina Zürbes, Nesrine Bali, Dušan Materić, Jan Willem Foppen","doi":"10.2166/aqua.2023.278","DOIUrl":null,"url":null,"abstract":"Abstract Nanoplastics are detected in surface water, yet accurately quantifying their particle number concentrations remains a significant challenge. In this study, we tested the applicability of a gold-labelling method to quantify nanoplastics in natural organic matter (NOM) containing water matrices. Gelatin-coated gold nanoparticles (Au-gel NPs) form conjugates with nanoplastics via electrostatic interaction which produces peak signals which can be translated into particle number concentration using single-particle inductively coupled plasma–mass spectrometry (SP-ICP-MS). We used water samples with various NOM concentrations, with and without the addition of 1 × 107 particles L−1 nanoplastics. Our results indicate that nanoplastics in low NOM samples (<1 mg·C L−1) could be successfully quantified. However, in high NOM samples (>15 mg·C L−1), only 13–19% of added nanoplastics were successfully quantified. Further digestion to remove NOM yielded only 10% of spiked nanoplastics. This discrepancy in high NOM samples could likely be attributed to the competition between nanoplastics and NOM existing in the water sample to bind with Au-gel NPs. Our study highlights the suitability of the Au-gel labelling method for quantifying nanoplastics in low NOM water samples. Nevertheless, further optimization, including pre-digestion steps, is essential to apply this method for high NOM water samples effectively.","PeriodicalId":34693,"journal":{"name":"AQUA-Water Infrastructure Ecosystems and Society","volume":"7 2","pages":"0"},"PeriodicalIF":2.1000,"publicationDate":"2023-11-13","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"How suitable is the gold-labelling method for the quantification of nanoplastics in natural water?\",\"authors\":\"Februriyana Pirade, Kim Lompe, Javier Jimenez-Lamana, Sulalit Bandyopadhyay, Katharina Zürbes, Nesrine Bali, Dušan Materić, Jan Willem Foppen\",\"doi\":\"10.2166/aqua.2023.278\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Abstract Nanoplastics are detected in surface water, yet accurately quantifying their particle number concentrations remains a significant challenge. In this study, we tested the applicability of a gold-labelling method to quantify nanoplastics in natural organic matter (NOM) containing water matrices. Gelatin-coated gold nanoparticles (Au-gel NPs) form conjugates with nanoplastics via electrostatic interaction which produces peak signals which can be translated into particle number concentration using single-particle inductively coupled plasma–mass spectrometry (SP-ICP-MS). We used water samples with various NOM concentrations, with and without the addition of 1 × 107 particles L−1 nanoplastics. Our results indicate that nanoplastics in low NOM samples (<1 mg·C L−1) could be successfully quantified. However, in high NOM samples (>15 mg·C L−1), only 13–19% of added nanoplastics were successfully quantified. Further digestion to remove NOM yielded only 10% of spiked nanoplastics. This discrepancy in high NOM samples could likely be attributed to the competition between nanoplastics and NOM existing in the water sample to bind with Au-gel NPs. Our study highlights the suitability of the Au-gel labelling method for quantifying nanoplastics in low NOM water samples. Nevertheless, further optimization, including pre-digestion steps, is essential to apply this method for high NOM water samples effectively.\",\"PeriodicalId\":34693,\"journal\":{\"name\":\"AQUA-Water Infrastructure Ecosystems and Society\",\"volume\":\"7 2\",\"pages\":\"0\"},\"PeriodicalIF\":2.1000,\"publicationDate\":\"2023-11-13\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"AQUA-Water Infrastructure Ecosystems and Society\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.2166/aqua.2023.278\",\"RegionNum\":4,\"RegionCategory\":\"环境科学与生态学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"ENGINEERING, CIVIL\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"AQUA-Water Infrastructure Ecosystems and Society","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.2166/aqua.2023.278","RegionNum":4,"RegionCategory":"环境科学与生态学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"ENGINEERING, CIVIL","Score":null,"Total":0}
How suitable is the gold-labelling method for the quantification of nanoplastics in natural water?
Abstract Nanoplastics are detected in surface water, yet accurately quantifying their particle number concentrations remains a significant challenge. In this study, we tested the applicability of a gold-labelling method to quantify nanoplastics in natural organic matter (NOM) containing water matrices. Gelatin-coated gold nanoparticles (Au-gel NPs) form conjugates with nanoplastics via electrostatic interaction which produces peak signals which can be translated into particle number concentration using single-particle inductively coupled plasma–mass spectrometry (SP-ICP-MS). We used water samples with various NOM concentrations, with and without the addition of 1 × 107 particles L−1 nanoplastics. Our results indicate that nanoplastics in low NOM samples (<1 mg·C L−1) could be successfully quantified. However, in high NOM samples (>15 mg·C L−1), only 13–19% of added nanoplastics were successfully quantified. Further digestion to remove NOM yielded only 10% of spiked nanoplastics. This discrepancy in high NOM samples could likely be attributed to the competition between nanoplastics and NOM existing in the water sample to bind with Au-gel NPs. Our study highlights the suitability of the Au-gel labelling method for quantifying nanoplastics in low NOM water samples. Nevertheless, further optimization, including pre-digestion steps, is essential to apply this method for high NOM water samples effectively.