{"title":"非创伤性修复中玻璃离子水门合剂的表面硬度","authors":"P. R. W. Barbosa, A. R. Lopes, L. M. S. Lima, M. Lima, A. Brandim, A. R. Gonçalves","doi":"10.4034/PBOCI.2016.161.47","DOIUrl":null,"url":null,"abstract":"Objective: To evaluate the surface hardness of a national glass ionomer cement with increased powder / liquid ratio, suitable for the atraumatic restorative treatment technique. Material and Methods: This is a study of the quantitative experimental type, in which 30 specimens were made and divided equally into 03 experimental groups (glass ionomer cement restorative Vitro Molar -DFL in the proportion specified by the manufacturer; glass ionomer cement restorative Vitro molar ratio -DFL modified with incorporation of 50% powder; and Gold Label 9 - GC Corporation in the proportion specified by the manufacturer). After handling, the materials were placed in a Teflon mold for manufacturing the cylindrical samples (5mm x 2 mm), with the aid of a Centrix syringe (Centrix, Shelton, CT, USA). Specimens were stored in liquid petroleum jelly at a temperature 37 ° ± 1 for up to 7 days. The specimens were evaluated by Vickers hardness test at time intervals of 24 hours and 7 days after manufacture. The data were subjected to the Independent Student’s-t tests and analysis of variance (ANOVA), and subsequently by Tukey's test at 95% level of significance. Results: The setting time positively influenced the hardness of the two glass ionomer cements (p<0,001). Cement Gold Label 9 showed higher hardness values than cement Vitro Molar (p<0,001), irrespective of the evaluation time interval. The latter in turn, showed improved values when manipulated with the modified powder / liquid ratio (3: 2) (p<0,001). Conclusion: Vitro Molar glass ionomer cement showed higher hardness values when manipulated with the modified powder/liquid ratio.","PeriodicalId":134552,"journal":{"name":"Brazilian Research in Pediatric Dentistry and Integrated Clinic","volume":"2 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2016-12-16","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"Surface Hardness of Glass Ionomer Cements used in Atraumatic Restorative Treatment\",\"authors\":\"P. R. W. Barbosa, A. R. Lopes, L. M. S. Lima, M. Lima, A. Brandim, A. R. Gonçalves\",\"doi\":\"10.4034/PBOCI.2016.161.47\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Objective: To evaluate the surface hardness of a national glass ionomer cement with increased powder / liquid ratio, suitable for the atraumatic restorative treatment technique. Material and Methods: This is a study of the quantitative experimental type, in which 30 specimens were made and divided equally into 03 experimental groups (glass ionomer cement restorative Vitro Molar -DFL in the proportion specified by the manufacturer; glass ionomer cement restorative Vitro molar ratio -DFL modified with incorporation of 50% powder; and Gold Label 9 - GC Corporation in the proportion specified by the manufacturer). After handling, the materials were placed in a Teflon mold for manufacturing the cylindrical samples (5mm x 2 mm), with the aid of a Centrix syringe (Centrix, Shelton, CT, USA). Specimens were stored in liquid petroleum jelly at a temperature 37 ° ± 1 for up to 7 days. The specimens were evaluated by Vickers hardness test at time intervals of 24 hours and 7 days after manufacture. The data were subjected to the Independent Student’s-t tests and analysis of variance (ANOVA), and subsequently by Tukey's test at 95% level of significance. Results: The setting time positively influenced the hardness of the two glass ionomer cements (p<0,001). Cement Gold Label 9 showed higher hardness values than cement Vitro Molar (p<0,001), irrespective of the evaluation time interval. The latter in turn, showed improved values when manipulated with the modified powder / liquid ratio (3: 2) (p<0,001). Conclusion: Vitro Molar glass ionomer cement showed higher hardness values when manipulated with the modified powder/liquid ratio.\",\"PeriodicalId\":134552,\"journal\":{\"name\":\"Brazilian Research in Pediatric Dentistry and Integrated Clinic\",\"volume\":\"2 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2016-12-16\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Brazilian Research in Pediatric Dentistry and Integrated Clinic\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.4034/PBOCI.2016.161.47\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Brazilian Research in Pediatric Dentistry and Integrated Clinic","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4034/PBOCI.2016.161.47","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

摘要

目的:评价一种粉液比增大的国产玻璃离子水门合剂的表面硬度,以适应非创伤性修复治疗技术。材料与方法:本研究为定量实验型研究,制作30个标本,按生产厂家规定的比例平均分为03个实验组(玻璃离子水门铁修复体体外磨牙-DFL);50%粉末掺入改性玻璃离子水泥修复体体外摩尔比;和金标9 - GC公司(按制造商指定的比例)。处理后,在Centrix注射器(Centrix, Shelton, CT, USA)的帮助下,将材料放置在聚四氟乙烯模具中以制造圆柱形样品(5mm x 2mm)。在37°±1温度下,凡士林液中保存7天。在制造后24小时和7天分别进行维氏硬度测试。数据采用独立学生t检验和方差分析(ANOVA),随后采用95%显著性水平的Tukey检验。结果:凝固时间对两种玻璃离子水门合剂的硬度有显著的正向影响(p< 0.001)。无论评估时间间隔如何,水泥金标9的硬度值高于水泥离体磨牙(p< 0.001)。当使用改良的粉液比(3:2)时,后者显示出改善的值(p< 0.001)。结论:改良粉液比后,体外磨牙玻璃离聚体水泥具有较高的硬度值。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Surface Hardness of Glass Ionomer Cements used in Atraumatic Restorative Treatment
Objective: To evaluate the surface hardness of a national glass ionomer cement with increased powder / liquid ratio, suitable for the atraumatic restorative treatment technique. Material and Methods: This is a study of the quantitative experimental type, in which 30 specimens were made and divided equally into 03 experimental groups (glass ionomer cement restorative Vitro Molar -DFL in the proportion specified by the manufacturer; glass ionomer cement restorative Vitro molar ratio -DFL modified with incorporation of 50% powder; and Gold Label 9 - GC Corporation in the proportion specified by the manufacturer). After handling, the materials were placed in a Teflon mold for manufacturing the cylindrical samples (5mm x 2 mm), with the aid of a Centrix syringe (Centrix, Shelton, CT, USA). Specimens were stored in liquid petroleum jelly at a temperature 37 ° ± 1 for up to 7 days. The specimens were evaluated by Vickers hardness test at time intervals of 24 hours and 7 days after manufacture. The data were subjected to the Independent Student’s-t tests and analysis of variance (ANOVA), and subsequently by Tukey's test at 95% level of significance. Results: The setting time positively influenced the hardness of the two glass ionomer cements (p<0,001). Cement Gold Label 9 showed higher hardness values than cement Vitro Molar (p<0,001), irrespective of the evaluation time interval. The latter in turn, showed improved values when manipulated with the modified powder / liquid ratio (3: 2) (p<0,001). Conclusion: Vitro Molar glass ionomer cement showed higher hardness values when manipulated with the modified powder/liquid ratio.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信