{"title":"用压力差加速脱毛","authors":"V. Valeika, V. Valeika","doi":"10.31554/978-5-7925-0601-5-2020-120-125","DOIUrl":null,"url":null,"abstract":"The method of accelerated unhairing without degrading the hair was stud-ied. The use of vacuum eliminated the influence of thickness on the penetration of unhairing solution. After speeding up the unhairing by vacuum and 12 hours of keeping of samples the strength of bond between hair and derma did not exceed 0,98 N. It means that hair can be removed by special mechanical means.","PeriodicalId":250562,"journal":{"name":"LEATHER AND FUR IN THE XXI CENTURY: TECHNOLOGY, QUALITY, ENVIRONMENTAL MANAGEMENT, EDUCATION","volume":"226 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"ACCELERATION OF UNHAIRING USING A DIFFERENCE OF PRESSURES\",\"authors\":\"V. Valeika, V. Valeika\",\"doi\":\"10.31554/978-5-7925-0601-5-2020-120-125\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The method of accelerated unhairing without degrading the hair was stud-ied. The use of vacuum eliminated the influence of thickness on the penetration of unhairing solution. After speeding up the unhairing by vacuum and 12 hours of keeping of samples the strength of bond between hair and derma did not exceed 0,98 N. It means that hair can be removed by special mechanical means.\",\"PeriodicalId\":250562,\"journal\":{\"name\":\"LEATHER AND FUR IN THE XXI CENTURY: TECHNOLOGY, QUALITY, ENVIRONMENTAL MANAGEMENT, EDUCATION\",\"volume\":\"226 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1900-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"LEATHER AND FUR IN THE XXI CENTURY: TECHNOLOGY, QUALITY, ENVIRONMENTAL MANAGEMENT, EDUCATION\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.31554/978-5-7925-0601-5-2020-120-125\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"LEATHER AND FUR IN THE XXI CENTURY: TECHNOLOGY, QUALITY, ENVIRONMENTAL MANAGEMENT, EDUCATION","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.31554/978-5-7925-0601-5-2020-120-125","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
ACCELERATION OF UNHAIRING USING A DIFFERENCE OF PRESSURES
The method of accelerated unhairing without degrading the hair was stud-ied. The use of vacuum eliminated the influence of thickness on the penetration of unhairing solution. After speeding up the unhairing by vacuum and 12 hours of keeping of samples the strength of bond between hair and derma did not exceed 0,98 N. It means that hair can be removed by special mechanical means.