输电线路断线热力学特性分析及金相检测

Sijin Cheng, Y. Zhou, Hao Sun, Junjian Tian, He Zhu, Jinfu Zhu, Hanliang Liao
{"title":"输电线路断线热力学特性分析及金相检测","authors":"Sijin Cheng, Y. Zhou, Hao Sun, Junjian Tian, He Zhu, Jinfu Zhu, Hanliang Liao","doi":"10.1145/3546000.3546030","DOIUrl":null,"url":null,"abstract":"In order to study the thermal mechanical characteristics of the broken line of the connecting pipe and pipeline joint of the transmission line, the tensile test of the steel cored aluminum strand steel wire, the thermodynamic analysis of the broken line joint of the connecting pipe and the metallographic test of the steel core of the broken line joint were carried out successively. The tensile strength of the steel core of the steel cored aluminum strand, the temperature load curve at different times and the metallographic test results of the steel core of the broken line joint were obtained, Finally, the exposed section of steel core is tested by metallography. The results show that the tensile strength of steel cored aluminum strand meets the standard, the heating of connecting pipe caused by conductor current will affect the calculated breaking force of steel core, and the exposed section of steel core has been running at high temperature for a period of time before being pulled off.","PeriodicalId":196955,"journal":{"name":"Proceedings of the 6th International Conference on High Performance Compilation, Computing and Communications","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2022-06-23","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Analysis of thermal-mechanical characteristics and metallographic detection of broken connection of transmission line\",\"authors\":\"Sijin Cheng, Y. Zhou, Hao Sun, Junjian Tian, He Zhu, Jinfu Zhu, Hanliang Liao\",\"doi\":\"10.1145/3546000.3546030\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In order to study the thermal mechanical characteristics of the broken line of the connecting pipe and pipeline joint of the transmission line, the tensile test of the steel cored aluminum strand steel wire, the thermodynamic analysis of the broken line joint of the connecting pipe and the metallographic test of the steel core of the broken line joint were carried out successively. The tensile strength of the steel core of the steel cored aluminum strand, the temperature load curve at different times and the metallographic test results of the steel core of the broken line joint were obtained, Finally, the exposed section of steel core is tested by metallography. The results show that the tensile strength of steel cored aluminum strand meets the standard, the heating of connecting pipe caused by conductor current will affect the calculated breaking force of steel core, and the exposed section of steel core has been running at high temperature for a period of time before being pulled off.\",\"PeriodicalId\":196955,\"journal\":{\"name\":\"Proceedings of the 6th International Conference on High Performance Compilation, Computing and Communications\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2022-06-23\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Proceedings of the 6th International Conference on High Performance Compilation, Computing and Communications\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1145/3546000.3546030\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Proceedings of the 6th International Conference on High Performance Compilation, Computing and Communications","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1145/3546000.3546030","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

为了研究输电线连接管断线和管道接头的热力学特性,先后进行了钢芯铝绞线钢丝的拉伸试验、连接管断线接头的热力学分析和断线接头钢芯的金相试验。获得了钢芯铝绞线钢芯的抗拉强度、不同时间的温度载荷曲线以及断线接头钢芯的金相试验结果,最后对钢芯裸露截面进行金相试验。结果表明:钢芯铝绞线的抗拉强度符合标准,导体电流引起的连接管发热会影响计算的钢芯断裂力,钢芯裸露段在高温下运行一段时间后才被拉断。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Analysis of thermal-mechanical characteristics and metallographic detection of broken connection of transmission line
In order to study the thermal mechanical characteristics of the broken line of the connecting pipe and pipeline joint of the transmission line, the tensile test of the steel cored aluminum strand steel wire, the thermodynamic analysis of the broken line joint of the connecting pipe and the metallographic test of the steel core of the broken line joint were carried out successively. The tensile strength of the steel core of the steel cored aluminum strand, the temperature load curve at different times and the metallographic test results of the steel core of the broken line joint were obtained, Finally, the exposed section of steel core is tested by metallography. The results show that the tensile strength of steel cored aluminum strand meets the standard, the heating of connecting pipe caused by conductor current will affect the calculated breaking force of steel core, and the exposed section of steel core has been running at high temperature for a period of time before being pulled off.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信