{"title":"[浸没试验中汞合金成分释放的毒理学评估]。","authors":"M Weiland,&nbsp;H Nossek","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>After immersion of unpolished and polished high copper amalgam in saliva with different pH values for up to 12 weeks, the elements mercury, tin, copper, silver and antimony were analysed in the solution. Unpolished amalgam corroded more than polished amalgam. Corrosion increased with the time of immersion and the acidity of the solution. The values calculated to a maximum of clinical application not imply any toxicologic risk.</p>","PeriodicalId":11244,"journal":{"name":"Deutsche zahnarztliche Zeitschrift","volume":"46 8","pages":"547-50"},"PeriodicalIF":0.0000,"publicationDate":"1991-08-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"[Toxicological assessment of amalgam components released in immersion tests].\",\"authors\":\"M Weiland,&nbsp;H Nossek\",\"doi\":\"\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>After immersion of unpolished and polished high copper amalgam in saliva with different pH values for up to 12 weeks, the elements mercury, tin, copper, silver and antimony were analysed in the solution. Unpolished amalgam corroded more than polished amalgam. Corrosion increased with the time of immersion and the acidity of the solution. The values calculated to a maximum of clinical application not imply any toxicologic risk.</p>\",\"PeriodicalId\":11244,\"journal\":{\"name\":\"Deutsche zahnarztliche Zeitschrift\",\"volume\":\"46 8\",\"pages\":\"547-50\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1991-08-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Deutsche zahnarztliche Zeitschrift\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Deutsche zahnarztliche Zeitschrift","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

将未抛光和抛光后的高铜汞合金浸泡在不同pH值的唾液中长达12周,分析了溶液中的汞、锡、铜、银和锑元素。未抛光的汞合金比抛光的汞合金更容易腐蚀。腐蚀随浸泡时间和溶液酸度的增加而增加。计算到临床应用最大值的数值并不意味着有任何毒理学风险。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
[Toxicological assessment of amalgam components released in immersion tests].

After immersion of unpolished and polished high copper amalgam in saliva with different pH values for up to 12 weeks, the elements mercury, tin, copper, silver and antimony were analysed in the solution. Unpolished amalgam corroded more than polished amalgam. Corrosion increased with the time of immersion and the acidity of the solution. The values calculated to a maximum of clinical application not imply any toxicologic risk.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信