{"title":"表面氟化硅橡胶的电晕老化和疏水性","authors":"Yujiao Tang, Z. An, F. Shan, F. Zheng, Yewen Zhang","doi":"10.1109/ICD.2016.7547694","DOIUrl":null,"url":null,"abstract":"We have reported that hydrophobicity of silicone rubber (SIR) can be significantly enhanced by direct fluorination. In this work, surface fluorinated SIR samples, together with the unfluorinated (virgin) ones were corona treated using a multi-needle-to-plate electrode system, to further evaluate corona resistance of the fluorinated SIR layer. ATR-IR analyses suggest that there may be oxidation of the partially fluorinated methyl groups and cleavage of Si-C bonds during the corona treatment, but the cleavage led to formation of Si-F bonds rather than Si-OH bonds. SEM surface and cross section images show that the corona treatment did not change the fluorinated layer thickness, although surface morphology was changed to some degree. In contrast with this, the virgin surface layer was severely degraded or ablated, forming a degraded layer on which aggregates of silica particles and/or degradation products of the SIR matrix material were left. Measurements of water contact angle and surface potential decay further confirm good resistance of the fluorinated layer to corona discharge.","PeriodicalId":306397,"journal":{"name":"2016 IEEE International Conference on Dielectrics (ICD)","volume":"47 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2016-07-03","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"4","resultStr":"{\"title\":\"Corona aging and hydrophobicity of surface fluorinated silicone rubbers\",\"authors\":\"Yujiao Tang, Z. An, F. Shan, F. Zheng, Yewen Zhang\",\"doi\":\"10.1109/ICD.2016.7547694\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"We have reported that hydrophobicity of silicone rubber (SIR) can be significantly enhanced by direct fluorination. In this work, surface fluorinated SIR samples, together with the unfluorinated (virgin) ones were corona treated using a multi-needle-to-plate electrode system, to further evaluate corona resistance of the fluorinated SIR layer. ATR-IR analyses suggest that there may be oxidation of the partially fluorinated methyl groups and cleavage of Si-C bonds during the corona treatment, but the cleavage led to formation of Si-F bonds rather than Si-OH bonds. SEM surface and cross section images show that the corona treatment did not change the fluorinated layer thickness, although surface morphology was changed to some degree. In contrast with this, the virgin surface layer was severely degraded or ablated, forming a degraded layer on which aggregates of silica particles and/or degradation products of the SIR matrix material were left. Measurements of water contact angle and surface potential decay further confirm good resistance of the fluorinated layer to corona discharge.\",\"PeriodicalId\":306397,\"journal\":{\"name\":\"2016 IEEE International Conference on Dielectrics (ICD)\",\"volume\":\"47 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2016-07-03\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"4\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2016 IEEE International Conference on Dielectrics (ICD)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/ICD.2016.7547694\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2016 IEEE International Conference on Dielectrics (ICD)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ICD.2016.7547694","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 4

摘要

我们报道了直接氟化可以显著提高硅橡胶(SIR)的疏水性。在这项工作中,使用多针-板电极系统对表面氟化SIR样品和未氟化SIR样品进行电晕处理,以进一步评估氟化SIR层的电晕电阻。ATR-IR分析表明,在电晕处理过程中,部分氟化甲基可能发生氧化,Si-C键断裂,但断裂导致Si-F键而不是Si-OH键的形成。SEM表面和截面图显示电晕处理没有改变氟化层的厚度,但表面形貌有一定程度的改变。与此相反,原始表面层被严重降解或烧蚀,形成一个降解层,上面留下二氧化硅颗粒聚集体和/或SIR基体材料的降解产物。水接触角和表面电位衰减的测量进一步证实了氟化层对电晕放电的良好抵抗能力。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Corona aging and hydrophobicity of surface fluorinated silicone rubbers
We have reported that hydrophobicity of silicone rubber (SIR) can be significantly enhanced by direct fluorination. In this work, surface fluorinated SIR samples, together with the unfluorinated (virgin) ones were corona treated using a multi-needle-to-plate electrode system, to further evaluate corona resistance of the fluorinated SIR layer. ATR-IR analyses suggest that there may be oxidation of the partially fluorinated methyl groups and cleavage of Si-C bonds during the corona treatment, but the cleavage led to formation of Si-F bonds rather than Si-OH bonds. SEM surface and cross section images show that the corona treatment did not change the fluorinated layer thickness, although surface morphology was changed to some degree. In contrast with this, the virgin surface layer was severely degraded or ablated, forming a degraded layer on which aggregates of silica particles and/or degradation products of the SIR matrix material were left. Measurements of water contact angle and surface potential decay further confirm good resistance of the fluorinated layer to corona discharge.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信