T Fuji, K Fujiwara, Y Hirata, T Hijikata, S Saito, K Ono
{"title":"熔喷氧化铝涂层金属植入物的体内固定评价——家兔实验。","authors":"T Fuji, K Fujiwara, Y Hirata, T Hijikata, S Saito, K Ono","doi":"","DOIUrl":null,"url":null,"abstract":"<p><p>Skeletal fixation characteristics of the stainless steel implants coated by 60 microns thick porous alumina layer using a flame spray method were evaluated in vivo for the duration of up to 12 weeks. Surface roughness of the implants appeared to be the determining factor for the fixation characteristics, irrespective of the implant materials.</p>","PeriodicalId":76134,"journal":{"name":"Medical journal of Osaka University","volume":"40 1-4","pages":"19-28"},"PeriodicalIF":0.0000,"publicationDate":"1991-03-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"In vivo evaluation of fixation of metal implants coated by melt-sprayed alumina--experiments in rabbit.\",\"authors\":\"T Fuji, K Fujiwara, Y Hirata, T Hijikata, S Saito, K Ono\",\"doi\":\"\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p><p>Skeletal fixation characteristics of the stainless steel implants coated by 60 microns thick porous alumina layer using a flame spray method were evaluated in vivo for the duration of up to 12 weeks. Surface roughness of the implants appeared to be the determining factor for the fixation characteristics, irrespective of the implant materials.</p>\",\"PeriodicalId\":76134,\"journal\":{\"name\":\"Medical journal of Osaka University\",\"volume\":\"40 1-4\",\"pages\":\"19-28\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1991-03-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Medical journal of Osaka University\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Medical journal of Osaka University","FirstCategoryId":"1085","ListUrlMain":"","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
In vivo evaluation of fixation of metal implants coated by melt-sprayed alumina--experiments in rabbit.
Skeletal fixation characteristics of the stainless steel implants coated by 60 microns thick porous alumina layer using a flame spray method were evaluated in vivo for the duration of up to 12 weeks. Surface roughness of the implants appeared to be the determining factor for the fixation characteristics, irrespective of the implant materials.