{"title":"掺锑氧化铁纳米颗粒的制备与表征","authors":"T. Jamal","doi":"10.52584/qrj.2101.08","DOIUrl":null,"url":null,"abstract":"Antimony oxide (Sb2O3) and Antimony-doped iron oxide (Sb-Fe2O3) nanomaterials of different (2 &3 %) concentrations were fabricated by wet synthesis technique and characterized by FTIR, XRD and XRF techniques, respectively. X-RD results showed uniform Iron oxide nanocrystals of almost 15 nm, whereas FTIR and XRF were employed to detect elemental composition of Antimony in doped (Sb-Fe2O3) samples.","PeriodicalId":426146,"journal":{"name":"Volume 21, Issue 1","volume":"116 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-06-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Fabrication and Characterization of Antimony doped Iron oxide Nanoparticles\",\"authors\":\"T. Jamal\",\"doi\":\"10.52584/qrj.2101.08\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Antimony oxide (Sb2O3) and Antimony-doped iron oxide (Sb-Fe2O3) nanomaterials of different (2 &3 %) concentrations were fabricated by wet synthesis technique and characterized by FTIR, XRD and XRF techniques, respectively. X-RD results showed uniform Iron oxide nanocrystals of almost 15 nm, whereas FTIR and XRF were employed to detect elemental composition of Antimony in doped (Sb-Fe2O3) samples.\",\"PeriodicalId\":426146,\"journal\":{\"name\":\"Volume 21, Issue 1\",\"volume\":\"116 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-06-30\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Volume 21, Issue 1\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.52584/qrj.2101.08\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Volume 21, Issue 1","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.52584/qrj.2101.08","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Fabrication and Characterization of Antimony doped Iron oxide Nanoparticles
Antimony oxide (Sb2O3) and Antimony-doped iron oxide (Sb-Fe2O3) nanomaterials of different (2 &3 %) concentrations were fabricated by wet synthesis technique and characterized by FTIR, XRD and XRF techniques, respectively. X-RD results showed uniform Iron oxide nanocrystals of almost 15 nm, whereas FTIR and XRF were employed to detect elemental composition of Antimony in doped (Sb-Fe2O3) samples.