{"title":"分子功能化的亲水石墨烯薄膜","authors":"Y. Taniguchi, T. Miki, Takanori Mitsuno, Y. Ohno, M. Nagase, K. Minagawa, M. Yasuzawa","doi":"10.1109/ICIPRM.2016.7528699","DOIUrl":null,"url":null,"abstract":"Hydrophilic graphene film by molecular functionalization was investigated. In order to realize the hydrophilic graphene film without introducing defects, the pyrene derivative with a phosphorylcholine group was synthesized. Functionalization time dependences on contact angle and 4-terminal resistivity were measured using SiC epitaxial graphene. Contact angle was almost constant (76°) at first, and then, suddenly decreased (59°) at 3 min. On the other hand, resistivity was gradually increased (0.6 to 2.4 μΩm), and saturated after 5 min, indicates that this functionalization process does not break the graphene structure. These results indicate that hydrophilic graphene film was successfully fabricated by molecular functionalization.","PeriodicalId":357009,"journal":{"name":"2016 Compound Semiconductor Week (CSW) [Includes 28th International Conference on Indium Phosphide & Related Materials (IPRM) & 43rd International Symposium on Compound Semiconductors (ISCS)","volume":"2 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2016-06-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Hydrophilic graphene film by molecular functionalization\",\"authors\":\"Y. Taniguchi, T. Miki, Takanori Mitsuno, Y. Ohno, M. Nagase, K. Minagawa, M. Yasuzawa\",\"doi\":\"10.1109/ICIPRM.2016.7528699\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Hydrophilic graphene film by molecular functionalization was investigated. In order to realize the hydrophilic graphene film without introducing defects, the pyrene derivative with a phosphorylcholine group was synthesized. Functionalization time dependences on contact angle and 4-terminal resistivity were measured using SiC epitaxial graphene. Contact angle was almost constant (76°) at first, and then, suddenly decreased (59°) at 3 min. On the other hand, resistivity was gradually increased (0.6 to 2.4 μΩm), and saturated after 5 min, indicates that this functionalization process does not break the graphene structure. These results indicate that hydrophilic graphene film was successfully fabricated by molecular functionalization.\",\"PeriodicalId\":357009,\"journal\":{\"name\":\"2016 Compound Semiconductor Week (CSW) [Includes 28th International Conference on Indium Phosphide & Related Materials (IPRM) & 43rd International Symposium on Compound Semiconductors (ISCS)\",\"volume\":\"2 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2016-06-26\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2016 Compound Semiconductor Week (CSW) [Includes 28th International Conference on Indium Phosphide & Related Materials (IPRM) & 43rd International Symposium on Compound Semiconductors (ISCS)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/ICIPRM.2016.7528699\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2016 Compound Semiconductor Week (CSW) [Includes 28th International Conference on Indium Phosphide & Related Materials (IPRM) & 43rd International Symposium on Compound Semiconductors (ISCS)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ICIPRM.2016.7528699","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

通过分子功能化研究了亲水石墨烯薄膜。为了实现不引入缺陷的亲水性石墨烯薄膜,合成了含磷胆碱基团的芘衍生物。利用SiC外延石墨烯测量了功能化时间对接触角和四端电阻率的依赖。接触角起初基本不变(76°),然后在3 min时突然减小(59°)。另一方面,电阻率逐渐增加(0.6 ~ 2.4 μΩm),并在5 min后饱和,表明这种功能化过程没有破坏石墨烯的结构。这些结果表明,通过分子功能化方法成功制备了亲水石墨烯薄膜。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Hydrophilic graphene film by molecular functionalization
Hydrophilic graphene film by molecular functionalization was investigated. In order to realize the hydrophilic graphene film without introducing defects, the pyrene derivative with a phosphorylcholine group was synthesized. Functionalization time dependences on contact angle and 4-terminal resistivity were measured using SiC epitaxial graphene. Contact angle was almost constant (76°) at first, and then, suddenly decreased (59°) at 3 min. On the other hand, resistivity was gradually increased (0.6 to 2.4 μΩm), and saturated after 5 min, indicates that this functionalization process does not break the graphene structure. These results indicate that hydrophilic graphene film was successfully fabricated by molecular functionalization.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信