{"title":"竹材-环氧复合材料管的破碎性能","authors":"Hadi Saputra, Jamasri., H. Rochardjo","doi":"10.1109/INAES.2017.8068567","DOIUrl":null,"url":null,"abstract":"An experimental investigation was conducted to study the crush-worthiness parameters and behaviour of the bamboo-epoxy composite tube with chamfering angle 45° at one end. Quasi-static compressive loadings were applied axially to investigate the response of force-displacement during progressive collapses. The Shimadzu concrete compression testing machine with capacity 2000 KN was used in this experiment. Load-displacement curve and collapses mode of the specimen are presented and discussed. The results showed that this novel uni-directional bamboo-fibers/epoxy tube could absorb 5.01 KJ energy caused by moving of cross head as far as 50 mm. The other crush-worthiness parameters are force average, crush force efficiency, and the specific energy absorption which have value of 102.60 KN, 0.57, and 18.23 KJ/kg, respectively. The progressive collapse mechanisms which occur in this experimental design are consisting of fragmentation and splaying failure modes. In conclusion, the results demonstrate a novel Crash box product constructed from bamboo and epoxy with good performance findings within crash-worthiness parameters comparing to the original equipment manufacturer product.","PeriodicalId":382919,"journal":{"name":"2017 7th International Annual Engineering Seminar (InAES)","volume":"91 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2017-08-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"The crushing behaviour of bamboo — Epoxy composite tube\",\"authors\":\"Hadi Saputra, Jamasri., H. Rochardjo\",\"doi\":\"10.1109/INAES.2017.8068567\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"An experimental investigation was conducted to study the crush-worthiness parameters and behaviour of the bamboo-epoxy composite tube with chamfering angle 45° at one end. Quasi-static compressive loadings were applied axially to investigate the response of force-displacement during progressive collapses. The Shimadzu concrete compression testing machine with capacity 2000 KN was used in this experiment. Load-displacement curve and collapses mode of the specimen are presented and discussed. The results showed that this novel uni-directional bamboo-fibers/epoxy tube could absorb 5.01 KJ energy caused by moving of cross head as far as 50 mm. The other crush-worthiness parameters are force average, crush force efficiency, and the specific energy absorption which have value of 102.60 KN, 0.57, and 18.23 KJ/kg, respectively. The progressive collapse mechanisms which occur in this experimental design are consisting of fragmentation and splaying failure modes. In conclusion, the results demonstrate a novel Crash box product constructed from bamboo and epoxy with good performance findings within crash-worthiness parameters comparing to the original equipment manufacturer product.\",\"PeriodicalId\":382919,\"journal\":{\"name\":\"2017 7th International Annual Engineering Seminar (InAES)\",\"volume\":\"91 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2017-08-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2017 7th International Annual Engineering Seminar (InAES)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/INAES.2017.8068567\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2017 7th International Annual Engineering Seminar (InAES)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/INAES.2017.8068567","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
The crushing behaviour of bamboo — Epoxy composite tube
An experimental investigation was conducted to study the crush-worthiness parameters and behaviour of the bamboo-epoxy composite tube with chamfering angle 45° at one end. Quasi-static compressive loadings were applied axially to investigate the response of force-displacement during progressive collapses. The Shimadzu concrete compression testing machine with capacity 2000 KN was used in this experiment. Load-displacement curve and collapses mode of the specimen are presented and discussed. The results showed that this novel uni-directional bamboo-fibers/epoxy tube could absorb 5.01 KJ energy caused by moving of cross head as far as 50 mm. The other crush-worthiness parameters are force average, crush force efficiency, and the specific energy absorption which have value of 102.60 KN, 0.57, and 18.23 KJ/kg, respectively. The progressive collapse mechanisms which occur in this experimental design are consisting of fragmentation and splaying failure modes. In conclusion, the results demonstrate a novel Crash box product constructed from bamboo and epoxy with good performance findings within crash-worthiness parameters comparing to the original equipment manufacturer product.