{"title":"纵切锯片有裂纹","authors":"F. Naumann, F. Spies","doi":"10.31399/asm.fach.machtools.c9001229","DOIUrl":null,"url":null,"abstract":"\n Two slitting saw blades were delivered for the purpose of determining the cause of damage. One had cracked while the other one came from a prior sheet delivery, that had less tendency to crack formation according to the manufacturer. The blades were supposed to have been stamped out of a sheet made from a 55 kp/sq mm strength steel. The saw blades were used for separating steel profiles at high rotational speeds. The cracks in question were located at the base of the teeth, i.e. at the point of highest operating stress. Metallographic examination showed that all cracks were non-decarburized and were free of chromium deposits. Therefore they could not have existed before heat treatment and chrome plating. It was concluded that the damage was due neither to poor quality of the sheet nor to defective stamping or heat treatment, but had occurred later either during surface treatment or during operation.","PeriodicalId":446028,"journal":{"name":"ASM Failure Analysis Case Histories: Machine Tools and Manufacturing Equipment","volume":"48 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2019-06-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Cracked Slitting Saw Blades\",\"authors\":\"F. Naumann, F. Spies\",\"doi\":\"10.31399/asm.fach.machtools.c9001229\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"\\n Two slitting saw blades were delivered for the purpose of determining the cause of damage. One had cracked while the other one came from a prior sheet delivery, that had less tendency to crack formation according to the manufacturer. The blades were supposed to have been stamped out of a sheet made from a 55 kp/sq mm strength steel. The saw blades were used for separating steel profiles at high rotational speeds. The cracks in question were located at the base of the teeth, i.e. at the point of highest operating stress. Metallographic examination showed that all cracks were non-decarburized and were free of chromium deposits. Therefore they could not have existed before heat treatment and chrome plating. It was concluded that the damage was due neither to poor quality of the sheet nor to defective stamping or heat treatment, but had occurred later either during surface treatment or during operation.\",\"PeriodicalId\":446028,\"journal\":{\"name\":\"ASM Failure Analysis Case Histories: Machine Tools and Manufacturing Equipment\",\"volume\":\"48 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2019-06-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"ASM Failure Analysis Case Histories: Machine Tools and Manufacturing Equipment\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.31399/asm.fach.machtools.c9001229\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"ASM Failure Analysis Case Histories: Machine Tools and Manufacturing Equipment","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.31399/asm.fach.machtools.c9001229","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

为了确定损坏的原因,送去了两个纵切锯片。一个已经破裂,而另一个来自以前的板材交付,有较少的倾向,裂纹形成根据制造商。这些叶片应该是用55 kp/sq mm强度的钢板冲压而成的。锯片用于高转速下钢型材的分离。所讨论的裂纹位于齿的基部,即在最高的工作应力点。金相检查表明,所有裂纹均未脱碳,无铬沉积。因此,在热处理和镀铬之前,它们不可能存在。结论是,损坏既不是由于板材质量差,也不是由于冲压或热处理有缺陷,而是在后来的表面处理或操作过程中发生的。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Cracked Slitting Saw Blades
Two slitting saw blades were delivered for the purpose of determining the cause of damage. One had cracked while the other one came from a prior sheet delivery, that had less tendency to crack formation according to the manufacturer. The blades were supposed to have been stamped out of a sheet made from a 55 kp/sq mm strength steel. The saw blades were used for separating steel profiles at high rotational speeds. The cracks in question were located at the base of the teeth, i.e. at the point of highest operating stress. Metallographic examination showed that all cracks were non-decarburized and were free of chromium deposits. Therefore they could not have existed before heat treatment and chrome plating. It was concluded that the damage was due neither to poor quality of the sheet nor to defective stamping or heat treatment, but had occurred later either during surface treatment or during operation.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信