{"title":"不锈钢焊缝堆焊层对API 5L管硬度的影响","authors":"Adhe Aryswan, Nurul Laili Arifin, Hanifah Widiastuti, Dois Ditya Wahyu Kirana","doi":"10.5220/0010352801190123","DOIUrl":null,"url":null,"abstract":": To improve the corrosion resistance of API 5 L pipe, we applied a weld overlay of UNS S31603 stainless steel as filler metal. To confirm the modified material’s quality, we determine the hardness of the material to be compared to API 5LD specification. We performed Vickers hardness tests at the corrosion-resistant alloy (CRA) area and the base metal and heat-affected zone. The tests show that the deposition improves the material hardness by 7.32%. The average Vickers hardness number at the CRA area was 212.32 HV, with 230 HV. Referring to API 5LD qualification, the maximum hardness allowed at the CRA area is 300 HV. Thus, the material processed by weld overlay has an acceptable quality.","PeriodicalId":103441,"journal":{"name":"Proceedings of the 3rd International Conference on Applied Engineering","volume":"156 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":"{\"title\":\"Effect of Stainless Steel Weld Overlay Deposit on the Hardness of API 5L Pipes\",\"authors\":\"Adhe Aryswan, Nurul Laili Arifin, Hanifah Widiastuti, Dois Ditya Wahyu Kirana\",\"doi\":\"10.5220/0010352801190123\",\"DOIUrl\":null,\"url\":null,\"abstract\":\": To improve the corrosion resistance of API 5 L pipe, we applied a weld overlay of UNS S31603 stainless steel as filler metal. To confirm the modified material’s quality, we determine the hardness of the material to be compared to API 5LD specification. We performed Vickers hardness tests at the corrosion-resistant alloy (CRA) area and the base metal and heat-affected zone. The tests show that the deposition improves the material hardness by 7.32%. The average Vickers hardness number at the CRA area was 212.32 HV, with 230 HV. Referring to API 5LD qualification, the maximum hardness allowed at the CRA area is 300 HV. Thus, the material processed by weld overlay has an acceptable quality.\",\"PeriodicalId\":103441,\"journal\":{\"name\":\"Proceedings of the 3rd International Conference on Applied Engineering\",\"volume\":\"156 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1900-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"3\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Proceedings of the 3rd International Conference on Applied Engineering\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.5220/0010352801190123\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Proceedings of the 3rd International Conference on Applied Engineering","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5220/0010352801190123","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

摘要

为了提高API 5l管的耐腐蚀性,我们采用了UNS S31603不锈钢作为填充金属的焊缝覆盖层。为了确认改性材料的质量,我们确定了要与API 5LD规范进行比较的材料的硬度。在耐腐蚀合金(CRA)区、母材和热影响区进行了维氏硬度测试。试验表明,沉积后的材料硬度提高了7.32%。CRA区的平均维氏硬度值为212.32 HV,最高为230 HV。参考API 5LD认证,CRA区域允许的最大硬度为300hv。因此,通过焊接覆盖处理的材料具有可接受的质量。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Effect of Stainless Steel Weld Overlay Deposit on the Hardness of API 5L Pipes
: To improve the corrosion resistance of API 5 L pipe, we applied a weld overlay of UNS S31603 stainless steel as filler metal. To confirm the modified material’s quality, we determine the hardness of the material to be compared to API 5LD specification. We performed Vickers hardness tests at the corrosion-resistant alloy (CRA) area and the base metal and heat-affected zone. The tests show that the deposition improves the material hardness by 7.32%. The average Vickers hardness number at the CRA area was 212.32 HV, with 230 HV. Referring to API 5LD qualification, the maximum hardness allowed at the CRA area is 300 HV. Thus, the material processed by weld overlay has an acceptable quality.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信