精加工和抛光程序对义齿基托树脂与两个长期弹性义齿衬垫之间间隙宽度的影响。

I. Pesun, J. Hodges, J. H. Lai
{"title":"精加工和抛光程序对义齿基托树脂与两个长期弹性义齿衬垫之间间隙宽度的影响。","authors":"I. Pesun, J. Hodges, J. H. Lai","doi":"10.1067/MPR.2002.122162","DOIUrl":null,"url":null,"abstract":"STATEMENT OF PROBLEM\nThe junction between a long-term, resilient denture liner and the denture base is difficult to finish and polish due to differences in the hardness of the materials. Gaps tend to form during finishing and polishing procedures.\n\n\nPURPOSE\nThis study measured the junctional gap between 2 long-term, resilient denture liners and a denture base material after different finishing and polishing procedures were performed. The surface smoothness of the 2 liner materials also was evaluated.\n\n\nMATERIAL AND METHODS\nMolloplast-B and an experimental, heat-polymerized methyl siloxane-resin-based denture liner were processed (according to the manufacturer's instructions) against Lucitone 199 acrylic resin. Control specimens (n = 20) were 2 mm thick and flat. Experimental specimens (n = 64) were fabricated with a raised center section: a 3- x 5- x 15-mm half-cylindrical ridge with a junction at the top of the cylinder between the liner material and acrylic resin. The specimens were finished with 1 of 6 types of burs and polished with different combinations of rubber-impregnated acrylic polishers, pumice, and tin oxide. The finished specimens were examined and photographed with a scanning electron microscope, and the largest gap along the liner/denture base junction on each specimen was measured. Three-way analysis of variance without replication (P<.05) and post-hoc t tests were used to analyze the data and compare groups. RESULTS; Averaged across finishing and polishing techniques, a larger gap was recorded for the experimental liner material (22 microm) than for Molloplast-B (14 microm) (P<.00005). Qualitative evaluation suggested that the experimental liner material polished better than Molloplast-B. The smoothest surfaces were obtained when specimens were finished with fine-tooth cross-cut carbide burs and polished with both pumice and tin oxide. A comparison between polished and unpolished specimens, averaged over materials and finishing techniques, revealed that polishing reduced gap size (P=.015).\n\n\nCONCLUSION\nWithin the limitations of this study, the 2 denture liners tested behaved similarly. The results suggest that the size of the gap at the liner/denture base junction may be affected by finishing and polishing techniques and vary among materials.","PeriodicalId":185384,"journal":{"name":"The Journal of prosthetic dentistry","volume":"2 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2002-03-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"16","resultStr":"{\"title\":\"Effect of finishing and polishing procedures on the gap width between a denture base resin and two long-term, resilient denture liners.\",\"authors\":\"I. Pesun, J. Hodges, J. H. Lai\",\"doi\":\"10.1067/MPR.2002.122162\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"STATEMENT OF PROBLEM\\nThe junction between a long-term, resilient denture liner and the denture base is difficult to finish and polish due to differences in the hardness of the materials. Gaps tend to form during finishing and polishing procedures.\\n\\n\\nPURPOSE\\nThis study measured the junctional gap between 2 long-term, resilient denture liners and a denture base material after different finishing and polishing procedures were performed. The surface smoothness of the 2 liner materials also was evaluated.\\n\\n\\nMATERIAL AND METHODS\\nMolloplast-B and an experimental, heat-polymerized methyl siloxane-resin-based denture liner were processed (according to the manufacturer's instructions) against Lucitone 199 acrylic resin. Control specimens (n = 20) were 2 mm thick and flat. Experimental specimens (n = 64) were fabricated with a raised center section: a 3- x 5- x 15-mm half-cylindrical ridge with a junction at the top of the cylinder between the liner material and acrylic resin. The specimens were finished with 1 of 6 types of burs and polished with different combinations of rubber-impregnated acrylic polishers, pumice, and tin oxide. The finished specimens were examined and photographed with a scanning electron microscope, and the largest gap along the liner/denture base junction on each specimen was measured. Three-way analysis of variance without replication (P<.05) and post-hoc t tests were used to analyze the data and compare groups. RESULTS; Averaged across finishing and polishing techniques, a larger gap was recorded for the experimental liner material (22 microm) than for Molloplast-B (14 microm) (P<.00005). Qualitative evaluation suggested that the experimental liner material polished better than Molloplast-B. The smoothest surfaces were obtained when specimens were finished with fine-tooth cross-cut carbide burs and polished with both pumice and tin oxide. A comparison between polished and unpolished specimens, averaged over materials and finishing techniques, revealed that polishing reduced gap size (P=.015).\\n\\n\\nCONCLUSION\\nWithin the limitations of this study, the 2 denture liners tested behaved similarly. The results suggest that the size of the gap at the liner/denture base junction may be affected by finishing and polishing techniques and vary among materials.\",\"PeriodicalId\":185384,\"journal\":{\"name\":\"The Journal of prosthetic dentistry\",\"volume\":\"2 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2002-03-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"16\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"The Journal of prosthetic dentistry\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1067/MPR.2002.122162\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"The Journal of prosthetic dentistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1067/MPR.2002.122162","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 16

摘要

问题陈述:由于材料的硬度差异,长期弹性义齿衬垫和义齿基托之间的连接处很难完成和抛光。在精加工和抛光过程中容易形成间隙。目的:本研究测量了两种长期弹性义齿衬垫与义齿基托材料在不同的整理和抛光过程后的连接间隙。对两种衬垫材料的表面光滑度进行了评价。材料和方法(根据制造商的说明)用Lucitone 199丙烯酸树脂对smolloplast -b和实验性热聚合甲基硅氧烷树脂基义齿衬垫进行处理。对照标本(n = 20)厚2 mm,呈扁平状。实验标本(n = 64)采用凸起的中心截面制作:一个3 × 5 × 15毫米的半圆柱形脊,在圆柱体的顶部有衬垫材料和丙烯酸树脂之间的连接处。这些标本用6种毛刺中的1种完成,并用浸渍橡胶的丙烯酸抛光剂、浮石和氧化锡的不同组合进行抛光。在扫描电子显微镜下检查和拍摄成品标本,并测量每个标本沿衬套/义齿基托连接处的最大间隙。采用无重复的三向方差分析(P< 0.05)和事后t检验进行数据分析和组间比较。结果;在精加工和抛光技术中平均,实验衬垫材料(22微米)比Molloplast-B(14微米)记录的间隙更大(P< 0.00005)。定性评价表明,实验衬垫材料抛光效果优于Molloplast-B。用细齿横切硬质合金毛刺和浮石和氧化锡抛光后,试样表面最光滑。抛光和未抛光样品之间的比较,根据材料和精加工技术的平均值,显示抛光减小了间隙尺寸(P= 0.015)。结论:在本研究的限制范围内,两种义齿衬垫的表现相似。结果表明,衬垫/义齿基托交界处的间隙大小可能受到抛光和抛光技术的影响,并且因材料而异。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Effect of finishing and polishing procedures on the gap width between a denture base resin and two long-term, resilient denture liners.
STATEMENT OF PROBLEM The junction between a long-term, resilient denture liner and the denture base is difficult to finish and polish due to differences in the hardness of the materials. Gaps tend to form during finishing and polishing procedures. PURPOSE This study measured the junctional gap between 2 long-term, resilient denture liners and a denture base material after different finishing and polishing procedures were performed. The surface smoothness of the 2 liner materials also was evaluated. MATERIAL AND METHODS Molloplast-B and an experimental, heat-polymerized methyl siloxane-resin-based denture liner were processed (according to the manufacturer's instructions) against Lucitone 199 acrylic resin. Control specimens (n = 20) were 2 mm thick and flat. Experimental specimens (n = 64) were fabricated with a raised center section: a 3- x 5- x 15-mm half-cylindrical ridge with a junction at the top of the cylinder between the liner material and acrylic resin. The specimens were finished with 1 of 6 types of burs and polished with different combinations of rubber-impregnated acrylic polishers, pumice, and tin oxide. The finished specimens were examined and photographed with a scanning electron microscope, and the largest gap along the liner/denture base junction on each specimen was measured. Three-way analysis of variance without replication (P<.05) and post-hoc t tests were used to analyze the data and compare groups. RESULTS; Averaged across finishing and polishing techniques, a larger gap was recorded for the experimental liner material (22 microm) than for Molloplast-B (14 microm) (P<.00005). Qualitative evaluation suggested that the experimental liner material polished better than Molloplast-B. The smoothest surfaces were obtained when specimens were finished with fine-tooth cross-cut carbide burs and polished with both pumice and tin oxide. A comparison between polished and unpolished specimens, averaged over materials and finishing techniques, revealed that polishing reduced gap size (P=.015). CONCLUSION Within the limitations of this study, the 2 denture liners tested behaved similarly. The results suggest that the size of the gap at the liner/denture base junction may be affected by finishing and polishing techniques and vary among materials.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信