{"title":"532nm,纳秒激光反射薄膜损伤竞赛","authors":"R. Negres, C. Stolz, G. Batavičiūtė, A. Melninkaitis","doi":"10.1117/12.2566691","DOIUrl":null,"url":null,"abstract":"This year’s competition aimed to survey state-of-the-art visible high reflectors in the nanosecond pulse length regime. The requirements for the coatings were a minimum reflection of 99.5% at 0 degrees incidence angle light at 532-nm. The choice of coating materials, design, and deposition method were left to the participants. Laser damage testing was performed at a single testing facility using the raster scanning test protocol with a 6-ns pulse length laser system operating at 100 Hz in a single-longitudinal mode. A double blind test assured sample and submitter anonymity. The damage performance results (LIDT), sample rankings, details of the deposition processes, coating materials and substrate cleaning methods are shared. We found that hafnia/silica multilayer coatings deposited by all five deposition methods surveyed were the most damage resistant within their group under these test conditions. In addition, hafnia/alumina/silica designs deposited performed second best.","PeriodicalId":202227,"journal":{"name":"Laser Damage","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2020-11-09","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"532-nm, nanosecond laser mirror thin film damage competition\",\"authors\":\"R. Negres, C. Stolz, G. Batavičiūtė, A. Melninkaitis\",\"doi\":\"10.1117/12.2566691\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"This year’s competition aimed to survey state-of-the-art visible high reflectors in the nanosecond pulse length regime. The requirements for the coatings were a minimum reflection of 99.5% at 0 degrees incidence angle light at 532-nm. The choice of coating materials, design, and deposition method were left to the participants. Laser damage testing was performed at a single testing facility using the raster scanning test protocol with a 6-ns pulse length laser system operating at 100 Hz in a single-longitudinal mode. A double blind test assured sample and submitter anonymity. The damage performance results (LIDT), sample rankings, details of the deposition processes, coating materials and substrate cleaning methods are shared. We found that hafnia/silica multilayer coatings deposited by all five deposition methods surveyed were the most damage resistant within their group under these test conditions. In addition, hafnia/alumina/silica designs deposited performed second best.\",\"PeriodicalId\":202227,\"journal\":{\"name\":\"Laser Damage\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-11-09\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Laser Damage\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1117/12.2566691\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Laser Damage","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1117/12.2566691","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

摘要

今年的竞赛旨在调查纳秒脉冲长度范围内最先进的可见高反射器。对涂层的要求是在532nm的0度入射角光线下,最低反射率为99.5%。涂层材料、设计和沉积方法的选择留给了参与者。激光损伤测试在单个测试设备上进行,使用光栅扫描测试协议,使用6 ns脉冲长度的激光系统,在单纵向模式下工作,频率为100 Hz。双盲测试保证了样本和提交者的匿名性。他们分享了损伤性能结果(LIDT)、样品排名、沉积过程细节、涂层材料和基材清洁方法。我们发现,在这些测试条件下,通过所有五种沉积方法沉积的铪/二氧化硅多层涂层是同类中最耐损伤的。此外,半氧化铪/氧化铝/二氧化硅设计的表现次之。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
532-nm, nanosecond laser mirror thin film damage competition
This year’s competition aimed to survey state-of-the-art visible high reflectors in the nanosecond pulse length regime. The requirements for the coatings were a minimum reflection of 99.5% at 0 degrees incidence angle light at 532-nm. The choice of coating materials, design, and deposition method were left to the participants. Laser damage testing was performed at a single testing facility using the raster scanning test protocol with a 6-ns pulse length laser system operating at 100 Hz in a single-longitudinal mode. A double blind test assured sample and submitter anonymity. The damage performance results (LIDT), sample rankings, details of the deposition processes, coating materials and substrate cleaning methods are shared. We found that hafnia/silica multilayer coatings deposited by all five deposition methods surveyed were the most damage resistant within their group under these test conditions. In addition, hafnia/alumina/silica designs deposited performed second best.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信