S. Gupta, A. Prasad, A. Chatterjee, Manoranjan Kumar, Somnath Ghosh, R. Datta
{"title":"Adoption of Sinter Addition in Steelmaking Converter to Control Spitting","authors":"S. Gupta, A. Prasad, A. Chatterjee, Manoranjan Kumar, Somnath Ghosh, R. Datta","doi":"10.1155/2015/187042","DOIUrl":null,"url":null,"abstract":"Steel Melting Shop-I, Rourkela Steel Plant, Rourkela, produces 0.5 MT of various special steels through BOF-VAR/VOR-LF-CC route. One of the most serious problems in BOF operations was lance skulling, hood jamming, and build-up of metal in the mouth and cone of the furnace due to spitting and slopping. As spitting occurring during blowing increases, these particles of metal are deposited inside the mouth and cone and affect badly BOF productivity. In the present work, control of spitting has been established by addition of sinter during the period of spitting. It also helped to improve the slag formation and fluidity of slag through increase of FeO content during peak decarburisation period.","PeriodicalId":16342,"journal":{"name":"Journal of Metallurgy","volume":"79 1","pages":"1-5"},"PeriodicalIF":0.0000,"publicationDate":"2015-12-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Metallurgy","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1155/2015/187042","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
Steel Melting Shop-I, Rourkela Steel Plant, Rourkela, produces 0.5 MT of various special steels through BOF-VAR/VOR-LF-CC route. One of the most serious problems in BOF operations was lance skulling, hood jamming, and build-up of metal in the mouth and cone of the furnace due to spitting and slopping. As spitting occurring during blowing increases, these particles of metal are deposited inside the mouth and cone and affect badly BOF productivity. In the present work, control of spitting has been established by addition of sinter during the period of spitting. It also helped to improve the slag formation and fluidity of slag through increase of FeO content during peak decarburisation period.