An investigation of the effect of methyl cellulose and sodium polyacrylate on the hydrosorption properties of a vulcanisate based on chloroprene rubber*

A. V. Ivanova, N. F. Ushmarin, E. Egorov, S. I. Sandalov, N. I. Kol’tsov
{"title":"An investigation of the effect of methyl cellulose and sodium polyacrylate on the hydrosorption properties of a vulcanisate based on chloroprene rubber*","authors":"A. V. Ivanova, N. F. Ushmarin, E. Egorov, S. I. Sandalov, N. I. Kol’tsov","doi":"10.1177/0307174X18450705","DOIUrl":null,"url":null,"abstract":"The effect of hydrophilic additives – MC-2000 methyl cellulose and sodium polyacrylate – on the properties of a vulcanisate based on Neoprene W was studied. The rubber mixes were prepared in two stages: at the first stage, hydrophilic additives were introduced into the rubber; at the second stage, the remaining ingredients were introduced. Vulcanisation was carried out at a temperature of 150°C for 30 min. The viscosity of the rubber mixes, M, was measured at 120°C on an MVR 3000 Basic viscometer (MonTech), and the vulcanisation characteristics and vulcanisation rate, v, were measured on an MDR 3000 Basic rheometer (MonTech) at 170°C in accordance with ASTM D2084-79. From the results of these measurements it follows that, with the combined use of methyl cellulose and sodium polyacrylate, there is a synergistic reduction in M and in the vulcanisation rate of the rubber mixes. A vulcanisate containing both hydrophilic additives possesses the best hydrosorption properties and has satisfactory physicomechanical properties (nominal tensile strength, elongation at break, hardness, and tear strength). The values of these properties and their changes on exposure of the vulcanisate to distilled water (70°C, 24 h) meet the requirements laid down for water-swelling rubber sealing elements.","PeriodicalId":14443,"journal":{"name":"International polymer science and technology","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2018-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International polymer science and technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1177/0307174X18450705","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

Abstract

The effect of hydrophilic additives – MC-2000 methyl cellulose and sodium polyacrylate – on the properties of a vulcanisate based on Neoprene W was studied. The rubber mixes were prepared in two stages: at the first stage, hydrophilic additives were introduced into the rubber; at the second stage, the remaining ingredients were introduced. Vulcanisation was carried out at a temperature of 150°C for 30 min. The viscosity of the rubber mixes, M, was measured at 120°C on an MVR 3000 Basic viscometer (MonTech), and the vulcanisation characteristics and vulcanisation rate, v, were measured on an MDR 3000 Basic rheometer (MonTech) at 170°C in accordance with ASTM D2084-79. From the results of these measurements it follows that, with the combined use of methyl cellulose and sodium polyacrylate, there is a synergistic reduction in M and in the vulcanisation rate of the rubber mixes. A vulcanisate containing both hydrophilic additives possesses the best hydrosorption properties and has satisfactory physicomechanical properties (nominal tensile strength, elongation at break, hardness, and tear strength). The values of these properties and their changes on exposure of the vulcanisate to distilled water (70°C, 24 h) meet the requirements laid down for water-swelling rubber sealing elements.
甲基纤维素和聚丙烯酸钠对氯丁橡胶基硫化胶吸氢性能影响的研究
研究了亲水性添加剂MC-2000甲基纤维素和聚丙烯酸钠对氯丁橡胶W基硫化胶性能的影响。胶料的制备分两个阶段:第一阶段,在胶料中加入亲水助剂;第二阶段,引入剩余配料。硫化在150°C的温度下进行30分钟。橡胶混合物的粘度M在120°C的MVR 3000基本粘度计(MonTech)上测量,硫化特性和硫化速率v在170°C的MDR 3000基本流变仪(MonTech)上根据ASTM D2084-79测量。从这些测量的结果可以得出,甲基纤维素和聚丙烯酸钠的联合使用,在M和橡胶混合物的硫化率有协同降低。含有这两种亲水性添加剂的硫化胶具有最佳的吸水性能,并具有令人满意的物理力学性能(标称抗拉强度、断裂伸长率、硬度和撕裂强度)。在蒸馏水中(70°C, 24小时),这些性能值及其变化符合遇水膨胀橡胶密封元件的要求。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信