{"title":"Evaluating the color stability of two esthetic ceramic materials after different surface treatments and accelerated aging procedures","authors":"Özge Gül, S. Agüloğlu","doi":"10.5577/intdentres.426","DOIUrl":null,"url":null,"abstract":"Aim: Observing and evaluating the long/short-term discoloration tendency of the esthetic prosthetic materials of lithium disilicate-based glass-ceramics (IPS e.max CAD LT) and leucite-based feldspathic glass-ceramics (VITA Mark II) materials, which are esthetically very close to each other at first glance. \nMethodology: 80 samples of A2 colored lithium disilicate and feldspathic blocks samples were overglazed and polished separately to evaluate the surface treatment procedures according to CIELAB color coordinates. For accelerated aging purposes, half of the examples were treated to red wine, and the other half were treated to coffee. Color changes were calculated using the ΔE formula. The results were put into record as ΔE-1, ΔE-2, and ΔE-3. Records of the results were evaluated using IBM SPSS Statistics Standard Concurrent User V 25 statistics package program. Data distribution regarding numerical variety and changes were evaluated using the Shapiro Wilk normality test and Q-Q graphics. \nResults: The data was evaluated using O'Brien clinical color tolerance scales. None of the samples has shown a perfect (ΔE=0-0.5) color match after 4 weeks of accelerated aging. Every group has shown results of significant statistical changes at various rates and percentages and divided into 4 subgroups as excellent, good, clinically acceptable and incompatible categories. \nConclusion: Since aging procedures affect ceramic systems' ΔE values in a variety of ways, the aging protocol utilizing in vitro aging techniques for color changing should be evaluated alongside ceramic type and surface finishing procedures. ","PeriodicalId":31322,"journal":{"name":"Journal of International Clinical Dental Research Organization","volume":null,"pages":null},"PeriodicalIF":0.2000,"publicationDate":"2022-10-26","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of International Clinical Dental Research Organization","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5577/intdentres.426","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0
Abstract
Aim: Observing and evaluating the long/short-term discoloration tendency of the esthetic prosthetic materials of lithium disilicate-based glass-ceramics (IPS e.max CAD LT) and leucite-based feldspathic glass-ceramics (VITA Mark II) materials, which are esthetically very close to each other at first glance.
Methodology: 80 samples of A2 colored lithium disilicate and feldspathic blocks samples were overglazed and polished separately to evaluate the surface treatment procedures according to CIELAB color coordinates. For accelerated aging purposes, half of the examples were treated to red wine, and the other half were treated to coffee. Color changes were calculated using the ΔE formula. The results were put into record as ΔE-1, ΔE-2, and ΔE-3. Records of the results were evaluated using IBM SPSS Statistics Standard Concurrent User V 25 statistics package program. Data distribution regarding numerical variety and changes were evaluated using the Shapiro Wilk normality test and Q-Q graphics.
Results: The data was evaluated using O'Brien clinical color tolerance scales. None of the samples has shown a perfect (ΔE=0-0.5) color match after 4 weeks of accelerated aging. Every group has shown results of significant statistical changes at various rates and percentages and divided into 4 subgroups as excellent, good, clinically acceptable and incompatible categories.
Conclusion: Since aging procedures affect ceramic systems' ΔE values in a variety of ways, the aging protocol utilizing in vitro aging techniques for color changing should be evaluated alongside ceramic type and surface finishing procedures.
目的:观察和评价二硅酸锂基微晶玻璃(IPS e.max CAD LT)和白晶石基长石微晶玻璃(VITA Mark II)材料的长/短期变色趋势,这两种材料乍一看在美学上非常接近。方法:分别对80个A2色二硅酸锂和长石块样品进行复釉和抛光,根据CIELAB颜色坐标对表面处理程序进行评价。为了加速老化的目的,一半的样本被处理成红酒,另一半被处理成咖啡。使用ΔE公式计算颜色变化。结果被记录为ΔE-1, ΔE-2和ΔE-3。使用IBM SPSS Statistics Standard Concurrent User v25统计包程序对结果记录进行评价。采用Shapiro Wilk正态性检验和Q-Q图对数值变化的数据分布进行评价。结果:采用O'Brien临床颜色耐受性量表对数据进行评估。经过4周的加速老化,没有一个样品显示出完美的颜色匹配(ΔE=0-0.5)。各组在不同的发生率和百分比上均显示出显著的统计学变化,并分为优、良、临床可接受和不相容4个亚组。结论:由于老化过程以多种方式影响陶瓷系统的ΔE值,因此应与陶瓷类型和表面处理过程一起评估利用体外老化技术进行颜色变化的老化方案。