{"title":"Research of the Composition of Phosphogypsum Produced During the Extracting of Phosphoric Acid from Ordinary Phosphorite Powder by the Clinker Method","authors":"B. Sultonov, A. A. Nodirov, D. S. Xolmatov","doi":"10.9734/csji/2023/v32i2844","DOIUrl":null,"url":null,"abstract":"In this article, processes of washing phosphogypsum with water, that formed during obtaining extractive phosphoric acid, by clinker method, from ordinary phosphorite powder (OPP) that is a raw material of Central Kyzylkum were studied. The phosphogypsum formed by washing a sample of phosphogypsum formed in 103% concentration of sulfuric acid without mixing with water, that obtained in the ratio OPP:H2O=1,0:2,5 was found to contain 2,55% P2O5, 29,90% CaO and 42,45% SO3. The acceptable sizes of washing the same phosphogypsum sample have been determined, mixing in different amounts of hot water. Phosphogypsum obtained in acceptable sizes contains 0,75% P2O5, 30,51% CaO and 43,58% SO3. When washing phosphogypsum samples with water, it saves 2.5 times the amount of water and causes to reduce the amount of P2O5 in its composition by at least 3 times. The amount of CaSO4 in the received phosphogypsum sample is increased from 79 to 86%. The samples of phosphogypsum formed without mixing with water and mixing with water were analyzed by X-ray phase analysis and their mutual salt contents were compared.","PeriodicalId":9803,"journal":{"name":"Chemical Science International Journal","volume":"137 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-04-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Chemical Science International Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.9734/csji/2023/v32i2844","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
In this article, processes of washing phosphogypsum with water, that formed during obtaining extractive phosphoric acid, by clinker method, from ordinary phosphorite powder (OPP) that is a raw material of Central Kyzylkum were studied. The phosphogypsum formed by washing a sample of phosphogypsum formed in 103% concentration of sulfuric acid without mixing with water, that obtained in the ratio OPP:H2O=1,0:2,5 was found to contain 2,55% P2O5, 29,90% CaO and 42,45% SO3. The acceptable sizes of washing the same phosphogypsum sample have been determined, mixing in different amounts of hot water. Phosphogypsum obtained in acceptable sizes contains 0,75% P2O5, 30,51% CaO and 43,58% SO3. When washing phosphogypsum samples with water, it saves 2.5 times the amount of water and causes to reduce the amount of P2O5 in its composition by at least 3 times. The amount of CaSO4 in the received phosphogypsum sample is increased from 79 to 86%. The samples of phosphogypsum formed without mixing with water and mixing with water were analyzed by X-ray phase analysis and their mutual salt contents were compared.