{"title":"Pemanfaatan Limbah Penggergajian Kayu Meranti Merah Sebagai Bahan Baku Papan Partikel Kerapatan Sedang Dengan Perekat Alami Asam Sitrat","authors":"D. N. Koroh, Mahdi Santoso, Fitri Diana Batubara, Milad Madiyawati, Nuwa Nuwa","doi":"10.36873/jht.v17i2.7537","DOIUrl":null,"url":null,"abstract":"Red Meranti was a commercial wood that is widely used as a raw material for the timber industry (plywood and sawmill industry), and generated a lot of waste. Currently, the utilization of red meranti waste has not been utilized optimally. One of the optimizing utilization of that waste was for developing a Particleboard with the citric acid natural binder. The objective of this study was to determine the bonding properties of Sawmill Waste Red Meranti Particleboard bonded with a Citric Acid Natural Adhesive. Citric acid was dissolved in water with the concentration of the solution adjusted to 60 wt%. This adhesive solution was sprayed onto the 40 mesh (coarse) and 40 mesh (fine) particles at 10% and 20% resin content based on the weight of oven-dried particles. Each mixture was then hot pressed at 110°C for 15 min under 50 kg/cm² pressure. Density and dimension targets were 0.7 kg/cm³; 30 × 30 × 1 cm. Each experiment was performed in triplicate, and the average value and standard deviation were calculated. The results showed that the interaction of particle size and adhesive content had a very significant effect on density, internal bonding, and screw-holding strength and had no significant effect on moisture content, thickness swelling, and modulus of rupture (MOR). Based on the SNI 03-2105-2006, the physical properties that meet the standard were moisture content and. Meanwhile, the mechanical properties of sawmill waste red meranti particleboard have not met the SNI 03-2105-2006. \nKata kunci (Keywords): Sawmill waste, red meranti waste, citric acid, natural binder.","PeriodicalId":42714,"journal":{"name":"Jurnal Manajemen Hutan Tropika","volume":null,"pages":null},"PeriodicalIF":0.4000,"publicationDate":"2022-12-03","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Manajemen Hutan Tropika","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.36873/jht.v17i2.7537","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"FORESTRY","Score":null,"Total":0}
引用次数: 0

Abstract

Red Meranti was a commercial wood that is widely used as a raw material for the timber industry (plywood and sawmill industry), and generated a lot of waste. Currently, the utilization of red meranti waste has not been utilized optimally. One of the optimizing utilization of that waste was for developing a Particleboard with the citric acid natural binder. The objective of this study was to determine the bonding properties of Sawmill Waste Red Meranti Particleboard bonded with a Citric Acid Natural Adhesive. Citric acid was dissolved in water with the concentration of the solution adjusted to 60 wt%. This adhesive solution was sprayed onto the 40 mesh (coarse) and 40 mesh (fine) particles at 10% and 20% resin content based on the weight of oven-dried particles. Each mixture was then hot pressed at 110°C for 15 min under 50 kg/cm² pressure. Density and dimension targets were 0.7 kg/cm³; 30 × 30 × 1 cm. Each experiment was performed in triplicate, and the average value and standard deviation were calculated. The results showed that the interaction of particle size and adhesive content had a very significant effect on density, internal bonding, and screw-holding strength and had no significant effect on moisture content, thickness swelling, and modulus of rupture (MOR). Based on the SNI 03-2105-2006, the physical properties that meet the standard were moisture content and. Meanwhile, the mechanical properties of sawmill waste red meranti particleboard have not met the SNI 03-2105-2006. Kata kunci (Keywords): Sawmill waste, red meranti waste, citric acid, natural binder.
采用红杉锯木厂作为密度铁胶板的成分与柠晶酸天然粘合剂使用
红莫兰蒂是一种商业木材,被广泛用作木材工业(胶合板和锯木厂工业)的原材料,产生了大量的废物。目前,红莫兰蒂废弃物的利用还没有得到最优的利用。其中一个优化利用的废物是开发一个刨花板与柠檬酸天然粘合剂。本研究的目的是确定锯木厂废红莫兰蒂刨花板与柠檬酸天然胶粘剂的粘合性能。柠檬酸溶于水,溶液浓度调至60%。根据烘箱干燥颗粒的重量,以10%和20%的树脂含量将该粘合剂溶液喷洒在40目(粗)和40目(细)颗粒上。然后在50 kg/cm²的压力下,在110°C下热压15分钟。密度和尺寸目标为0.7 kg/cm³;30 × 30 × 1厘米。每个实验做三次,计算平均值和标准差。结果表明:颗粒尺寸和黏合剂含量的交互作用对密度、内粘接和螺杆保持强度有非常显著的影响,而对含水率、厚度膨胀和断裂模量(MOR)没有显著影响。根据SNI 03-2105-2006,符合标准的物理性能为含水率和。同时,锯木厂废红莫兰蒂刨花板的力学性能不符合SNI标准03-2105-2006。关键词:锯木厂废料,红莫兰蒂废料,柠檬酸,天然粘合剂。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
CiteScore
1.80
自引率
20.00%
发文量
23
审稿时长
16 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信