Proton induced degradation of liquid phase crystallized poly-Si thin-film solar cells

Tim Frijnts, C. Pellegrino, S. Gall, H. Neitzert
{"title":"Proton induced degradation of liquid phase crystallized poly-Si thin-film solar cells","authors":"Tim Frijnts, C. Pellegrino, S. Gall, H. Neitzert","doi":"10.1109/PVSC45281.2020.9300392","DOIUrl":null,"url":null,"abstract":"Liquid phase crystallized poly-Si thin-film solar cells on glass with a-Si heterojunction emitters were irradiated with 68 MeV protons with different fluences up to 1013 protons/cm2. The degradation of devices with n-type and p-type absorber has been compared. A significantly stronger decrease of the solar cell performance parameters for devices with n-type absorber has been observed as compared to the p-type absorber case. This result corresponds to the different decrease of the minority carrier diffusion lengths with regard to the different poly-Si absorber materials.","PeriodicalId":6773,"journal":{"name":"2020 47th IEEE Photovoltaic Specialists Conference (PVSC)","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2020-06-14","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2020 47th IEEE Photovoltaic Specialists Conference (PVSC)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/PVSC45281.2020.9300392","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Liquid phase crystallized poly-Si thin-film solar cells on glass with a-Si heterojunction emitters were irradiated with 68 MeV protons with different fluences up to 1013 protons/cm2. The degradation of devices with n-type and p-type absorber has been compared. A significantly stronger decrease of the solar cell performance parameters for devices with n-type absorber has been observed as compared to the p-type absorber case. This result corresponds to the different decrease of the minority carrier diffusion lengths with regard to the different poly-Si absorber materials.
质子诱导降解液相结晶多晶硅薄膜太阳能电池
采用a-Si异质结发射体对玻璃上的液相结晶多晶硅薄膜太阳能电池进行68 MeV质子辐照,辐照强度可达1013个质子/cm2。比较了n型和p型吸收器器件的退化情况。与p型吸收体相比,n型吸收体的太阳能电池性能参数明显下降。这一结果对应于不同的多晶硅吸收材料对少数载流子扩散长度减小的不同。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信