{"title":"Properties of the polyacrylic acid resin duolite es 346 containing amidoxime anchor groups with respect to the separation of uranium from sea water","authors":"K. Lieser, M. Erboy, B. Thybusch","doi":"10.1002/APMC.1987.051520115","DOIUrl":null,"url":null,"abstract":"Loading curves, rate of exchange and distribution coefficients of Duolite ES 346 are determined for UO22+, Cu2+ and Fe3+, using simulated sea water. The crude resin gives off ammonia into solution which leads to precipitation of uranyl ions and high apparent distribution coefficients. With the purified resin the following distribution coefficients are measured at pH 8.1: Kd(UO22+) ≈ Kd(Cu2+) ≈ Kd(Fe3+) ≈ 0.6 · 104 ml/g. This leads to a loading of the resin in sea water of pH 8.1 with uranium only to about 20 μg per g of resin. \n \n \n \nDie Beladungskurven, die Austauschgeschwindigkeit und die Verteilungskoeffizienten von Duolit ES 346 wurden unter Verwendung von simuliertem Meerwasser fur UO22+, Cu2+ und Fe3+ bestimmt. Das rohe Harz gibt Ammoniak in die Losung ab, was zur Ausfallung von Uranylionen und scheinbar hohen Verteilungskoeffizienten fuhrt. Fur das gereinigte Harz wurden die folgenden Verteilungskoeffizienten bei pH 8,1 gemessen: Kd(UO22+) ≈ Kd(Cu2+) ≈ Kd(Fe3+) ≈ 0,6 · 104 ml/g. Dies fuhrt zu einer Beladung des Harzes in Meerwasser vom pH 8,1 mit Uran bis etwa 20 μg pro g Harz.","PeriodicalId":7808,"journal":{"name":"Angewandte Makromolekulare Chemie","volume":"89 1","pages":"169-178"},"PeriodicalIF":0.0000,"publicationDate":"1987-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"9","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Angewandte Makromolekulare Chemie","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1002/APMC.1987.051520115","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 9
Abstract
Loading curves, rate of exchange and distribution coefficients of Duolite ES 346 are determined for UO22+, Cu2+ and Fe3+, using simulated sea water. The crude resin gives off ammonia into solution which leads to precipitation of uranyl ions and high apparent distribution coefficients. With the purified resin the following distribution coefficients are measured at pH 8.1: Kd(UO22+) ≈ Kd(Cu2+) ≈ Kd(Fe3+) ≈ 0.6 · 104 ml/g. This leads to a loading of the resin in sea water of pH 8.1 with uranium only to about 20 μg per g of resin.
Die Beladungskurven, die Austauschgeschwindigkeit und die Verteilungskoeffizienten von Duolit ES 346 wurden unter Verwendung von simuliertem Meerwasser fur UO22+, Cu2+ und Fe3+ bestimmt. Das rohe Harz gibt Ammoniak in die Losung ab, was zur Ausfallung von Uranylionen und scheinbar hohen Verteilungskoeffizienten fuhrt. Fur das gereinigte Harz wurden die folgenden Verteilungskoeffizienten bei pH 8,1 gemessen: Kd(UO22+) ≈ Kd(Cu2+) ≈ Kd(Fe3+) ≈ 0,6 · 104 ml/g. Dies fuhrt zu einer Beladung des Harzes in Meerwasser vom pH 8,1 mit Uran bis etwa 20 μg pro g Harz.