Porous Cordierite Ceramics from Natural Clays / Poraina kordierīta keramika no dabiskiem māliem

M. Rundans, I. Šperberga
{"title":"Porous Cordierite Ceramics from Natural Clays / Poraina kordierīta keramika no dabiskiem māliem","authors":"M. Rundans, I. Šperberga","doi":"10.1515/msac-2015-0006","DOIUrl":null,"url":null,"abstract":"Abstract In this report the obtaining and properties of hightemperature porous ceramic materials using local carbonate clays and quartz sand resources was studied. Materials with two different porosities were obtained by using different synthesis temperatures. The test results show that these materials contain cordierite as their main crystalline phase. The porosity directly influences the compressive strength and it is greatly reduced when overall porosity increases. The CTE of obtained materials is low − about 3-10−6 1/°C. Keramikas materiāliem, kas veidoti sistēmā MgO-Al2O3-SiO2 ir plašs pielietojums dažādās jomās. Tā tas, piemēram, ir termiski stabilajai fāzei kordierītam (2MgO·2Al2O3·5SiO2). Kordierīta keramika ar tās zemo termiskās izplešanās koeficientu - TIK (α ≈ 1,0·10−6 -4,0·10−6 1/°C) droši iztur straujas temperatūras izmaiņas, tāpēc tā var tikt izmantota kā ugunsizturīgs materiāls. Dabā kordierīts ir reti sastopams minerāls, tādēļ šis kristāliskais materiāls ir jāiegūst sintētiski. Visplašāk izmantotā metode ir augsttemperatūras cietfāžu sintēze, retāk - sola-gēla sintēze un rekristalizācija no stiklveida kausējuma. Sintēzei tiek izmantotas dažādas magnija, alumīnija un silīcija oksīdus saturošas izejvielas, no kurām visbiežāk lietotās ir talks un kaolīns. Lai samazinātu nepieciešamo sintēzes temperatūru, oksīda maisījumiem tiek pievienoti dažādi kušņi, piemēram, B2O3. Šajā pētījumā ieguva augsti porainus kordierīta keramiskos materiālus, izmantojot vietējās izejvielas - karbonātu mālu un kvarca smiltis. Ieguva dažādas porainības materiālus, mainot sintēzes temperatūru. Rentgenfāžu analīzes rezultāti liecināja, ka šie materiāli saturēja kordierītu kā galveno kristālisko fāzi. Porainībai palielinoties, tā tieši ietekmēja spiedes stiprību, to ievērojami samazinot. Iegūto materiālu termiskās izplešanās koeficienti bija zemi (ne augstāki par 3,0·10−6 1/°C visā pētītajā temperatūras diapazonā), neskatoties uz poru un stiklveida fāzes klātbūtni.","PeriodicalId":18239,"journal":{"name":"Materials Science and Applied Chemistry","volume":"11 1","pages":"33 - 38"},"PeriodicalIF":0.0000,"publicationDate":"2015-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials Science and Applied Chemistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1515/msac-2015-0006","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

Abstract

Abstract In this report the obtaining and properties of hightemperature porous ceramic materials using local carbonate clays and quartz sand resources was studied. Materials with two different porosities were obtained by using different synthesis temperatures. The test results show that these materials contain cordierite as their main crystalline phase. The porosity directly influences the compressive strength and it is greatly reduced when overall porosity increases. The CTE of obtained materials is low − about 3-10−6 1/°C. Keramikas materiāliem, kas veidoti sistēmā MgO-Al2O3-SiO2 ir plašs pielietojums dažādās jomās. Tā tas, piemēram, ir termiski stabilajai fāzei kordierītam (2MgO·2Al2O3·5SiO2). Kordierīta keramika ar tās zemo termiskās izplešanās koeficientu - TIK (α ≈ 1,0·10−6 -4,0·10−6 1/°C) droši iztur straujas temperatūras izmaiņas, tāpēc tā var tikt izmantota kā ugunsizturīgs materiāls. Dabā kordierīts ir reti sastopams minerāls, tādēļ šis kristāliskais materiāls ir jāiegūst sintētiski. Visplašāk izmantotā metode ir augsttemperatūras cietfāžu sintēze, retāk - sola-gēla sintēze un rekristalizācija no stiklveida kausējuma. Sintēzei tiek izmantotas dažādas magnija, alumīnija un silīcija oksīdus saturošas izejvielas, no kurām visbiežāk lietotās ir talks un kaolīns. Lai samazinātu nepieciešamo sintēzes temperatūru, oksīda maisījumiem tiek pievienoti dažādi kušņi, piemēram, B2O3. Šajā pētījumā ieguva augsti porainus kordierīta keramiskos materiālus, izmantojot vietējās izejvielas - karbonātu mālu un kvarca smiltis. Ieguva dažādas porainības materiālus, mainot sintēzes temperatūru. Rentgenfāžu analīzes rezultāti liecināja, ka šie materiāli saturēja kordierītu kā galveno kristālisko fāzi. Porainībai palielinoties, tā tieši ietekmēja spiedes stiprību, to ievērojami samazinot. Iegūto materiālu termiskās izplešanās koeficienti bija zemi (ne augstāki par 3,0·10−6 1/°C visā pētītajā temperatūras diapazonā), neskatoties uz poru un stiklveida fāzes klātbūtni.
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信