Interplay between resin cements and surface-treated Poly-Ether-Ether-Ketone (PEEK)

Q4 Dentistry
A. Joly, Guilherme da Gama Ramos, C. Turssi
{"title":"Interplay between resin cements and surface-treated Poly-Ether-Ether-Ketone (PEEK)","authors":"A. Joly, Guilherme da Gama Ramos, C. Turssi","doi":"10.20396/bjos.v22i00.8670130","DOIUrl":null,"url":null,"abstract":"Aim: This study assessed the effect of thermal aging on the interfacial strength of resin cements to surface-treated PEEK. Methods: Ninety-six PEEK blocks were allocated into 4 groups (n=24), according to following surface treatments: SB - sandblasting with aluminum oxide; SA - acid etched with 98% sulfuric acid; CA – coupling agent (Visio.link, Bredent) and CO - control group (untreated). Surface roughness (Ra) was measured and one cylinder (1-mm diameter and height) of Rely-X Ultimate - ULT (3M/ESPE) and another one of Panavia V5 - PAN (Kuraray) were constructed on the treated or untreated PEEK surfaces. Half of the samples of each group were thermal aged (1,000 cycles). Samples were tested at a crosshead speed of 1 mm/min in shear mode (μSBS). Ra and μSBS data were compared using one- and three-way ANOVA, respectively, and Tukey’s tests. Results: SA and SB samples had the roughest surfaces, while CA the smoother (p<0.001). Thermal aging reduced μSBS regardless the surface treatment and resin cement used. There was interaction between surface treatment and resin cement (p <0.001), with ULT showing higher μSBS values than PAN. SA provided higher μSBS than SB for both resin cements, while for CA μSBS was higher (PAN) or lower than SB (ULT). Conclusion: Aging inadvertently reduces interfacial strength between PEEK and the resin cements. If ULT is the resin cement of choice, reliable interfacial strength is reached after any PEEK surface treatment. However, if PAN is going to be used only SA and CA are recommended as PEEK treatment.","PeriodicalId":34984,"journal":{"name":"Brazilian Journal of Oral Sciences","volume":"26 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-07-10","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Brazilian Journal of Oral Sciences","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.20396/bjos.v22i00.8670130","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"Dentistry","Score":null,"Total":0}
引用次数: 0

Abstract

Aim: This study assessed the effect of thermal aging on the interfacial strength of resin cements to surface-treated PEEK. Methods: Ninety-six PEEK blocks were allocated into 4 groups (n=24), according to following surface treatments: SB - sandblasting with aluminum oxide; SA - acid etched with 98% sulfuric acid; CA – coupling agent (Visio.link, Bredent) and CO - control group (untreated). Surface roughness (Ra) was measured and one cylinder (1-mm diameter and height) of Rely-X Ultimate - ULT (3M/ESPE) and another one of Panavia V5 - PAN (Kuraray) were constructed on the treated or untreated PEEK surfaces. Half of the samples of each group were thermal aged (1,000 cycles). Samples were tested at a crosshead speed of 1 mm/min in shear mode (μSBS). Ra and μSBS data were compared using one- and three-way ANOVA, respectively, and Tukey’s tests. Results: SA and SB samples had the roughest surfaces, while CA the smoother (p<0.001). Thermal aging reduced μSBS regardless the surface treatment and resin cement used. There was interaction between surface treatment and resin cement (p <0.001), with ULT showing higher μSBS values than PAN. SA provided higher μSBS than SB for both resin cements, while for CA μSBS was higher (PAN) or lower than SB (ULT). Conclusion: Aging inadvertently reduces interfacial strength between PEEK and the resin cements. If ULT is the resin cement of choice, reliable interfacial strength is reached after any PEEK surface treatment. However, if PAN is going to be used only SA and CA are recommended as PEEK treatment.
树脂胶结剂与表面处理聚醚-醚酮(PEEK)的相互作用
目的:研究热老化对表面处理PEEK树脂胶结物界面强度的影响。方法:96块聚醚醚酮砌块分为4组(n=24),表面处理:SB -氧化铝喷砂;SA -酸蚀刻用98%硫酸;CA偶联剂(Visio)link, brendent)和CO对照组(未经治疗)。测量表面粗糙度(Ra),并在处理或未处理的PEEK表面上构建一个圆柱体(直径和高度为1mm)的Rely-X Ultimate - ULT (3M/ESPE)和另一个Panavia V5 - PAN (Kuraray)。每组一半的样品进行热老化(1000次循环)。试样在剪切模式下以1 mm/min的十字速度(μSBS)进行测试。Ra和μSBS数据分别采用单因素和三因素方差分析和Tukey检验进行比较。结果:SA和SB样品表面最粗糙,CA样品表面较光滑(p<0.001)。无论表面处理和树脂水泥的使用,热老化都降低了μSBS。表面处理与树脂水泥之间存在交互作用(p <0.001),其中ULT的μSBS值高于PAN。SA对两种树脂胶结物的μSBS均高于SB,而CA的μSBS高于(PAN)或低于SB (ULT)。结论:老化无意中降低了PEEK与树脂胶结物之间的界面强度。如果选择ULT树脂水泥,则在任何PEEK表面处理后都能达到可靠的界面强度。但是,如果要使用PAN,则建议仅使用SA和CA作为PEEK处理。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Brazilian Journal of Oral Sciences
Brazilian Journal of Oral Sciences Dentistry-Dentistry (all)
CiteScore
0.60
自引率
0.00%
发文量
52
审稿时长
20 weeks
期刊介绍: The Brazilian Journal of Oral Sciences is an international non-profit journal, which publishes full-Length papers, original research reports, literature reviews, special reports, clinical cases, current topics and short communications, dealing with dentistry or related disciplines.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信