{"title":"Thermodynamic calculations for the formation of SiC-whisker-reinforced Si sub 3 N sub 4 ceramics","authors":"K. Nickel, M. Hoffmann, P. Greil, G. Petzow","doi":"10.1111/J.1551-2916.1988.TB00278.X","DOIUrl":null,"url":null,"abstract":"Thermodynamic equilibria were calculated to determine optimum fabrication conditions for SiC-whisker-reinforced Si{sub 3}N{sub 4} composite ceramics. Results of calculations indicate that pressureless sintering in a nitrogen atmosphere of 0.1 MPa may be performed at temperatures up to 2,123 K (1,850{degree}C) without whisker or matrix degradation. In addition, gas pressure sintering at temperatures up to 2,373 K (2,100{degree}C) requires a nitrogen pressure of 1 to 10 MPa. Hot isostatic pressing (total pressure {ge} 100 MPa) at 2,273 K (2,000{degree}C) can yield undegraded composite materials only when the nitrogen partial pressure in a gas mixture with an inert gas is kept between 1 to 10 MPa.","PeriodicalId":7260,"journal":{"name":"Advanced Ceramic Materials","volume":"42 1","pages":"557-562"},"PeriodicalIF":0.0000,"publicationDate":"1988-11-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"39","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Advanced Ceramic Materials","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1111/J.1551-2916.1988.TB00278.X","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 39
Abstract
Thermodynamic equilibria were calculated to determine optimum fabrication conditions for SiC-whisker-reinforced Si{sub 3}N{sub 4} composite ceramics. Results of calculations indicate that pressureless sintering in a nitrogen atmosphere of 0.1 MPa may be performed at temperatures up to 2,123 K (1,850{degree}C) without whisker or matrix degradation. In addition, gas pressure sintering at temperatures up to 2,373 K (2,100{degree}C) requires a nitrogen pressure of 1 to 10 MPa. Hot isostatic pressing (total pressure {ge} 100 MPa) at 2,273 K (2,000{degree}C) can yield undegraded composite materials only when the nitrogen partial pressure in a gas mixture with an inert gas is kept between 1 to 10 MPa.