Comparative study of different bis-citraconimides as anti-reversion agents in natural rubber

Mingbin He, Lijing Zou, Zhaohui Chen, Ruoming Huang
{"title":"Comparative study of different bis-citraconimides as anti-reversion agents in natural rubber","authors":"Mingbin He, Lijing Zou, Zhaohui Chen, Ruoming Huang","doi":"10.1177/00952443221138914","DOIUrl":null,"url":null,"abstract":"Sulfur-cured natural rubber (NR) commonly accompanies reversion, which severely impacts the properties as well as service life of NR products. Introducing anti-reversion agents is one of the most effective ways to counteract reversion. In this work, five structurally different bis-citraconimides have been synthesized and used as anti-reversion agents for sulfur-cured NR. In detail, the differences of anti-reversion agents in the cure characteristics, cross-linked structure, physical-mechanical properties, heat build-up, and dynamic mechanical properties of sulfur-cured NR are investigated in order to elaborate on the differences in reactivity and cross-linking chemistry of anti-reversion agents. The results show that N,N′-p-phenylene-biscitraconimide (BCmB) provides the best anti-reversion performance for compound cured at 150°C, with N,N′-p-phenylene-biscitraconimide (BCpB) following closely behind. Although Perkalink 900 (1,3-bis(citraconimidomethyl)benzene: BCDB), 1,3-bis(citraconimido)isobutane (BIB), and 1,6-bis(citraconimido)hexane (BCH) are less effective than BCmB and BCpB in improving the anti-reversion performance of compound cured for a short period of time or cured at 150°C, they show better anti-reversion performance of compound cured for a longer time or cured at higher vulcanization temperature.","PeriodicalId":15613,"journal":{"name":"Journal of Elastomers & Plastics","volume":"20 1","pages":"46 - 66"},"PeriodicalIF":0.0000,"publicationDate":"2022-11-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Elastomers & Plastics","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1177/00952443221138914","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Sulfur-cured natural rubber (NR) commonly accompanies reversion, which severely impacts the properties as well as service life of NR products. Introducing anti-reversion agents is one of the most effective ways to counteract reversion. In this work, five structurally different bis-citraconimides have been synthesized and used as anti-reversion agents for sulfur-cured NR. In detail, the differences of anti-reversion agents in the cure characteristics, cross-linked structure, physical-mechanical properties, heat build-up, and dynamic mechanical properties of sulfur-cured NR are investigated in order to elaborate on the differences in reactivity and cross-linking chemistry of anti-reversion agents. The results show that N,N′-p-phenylene-biscitraconimide (BCmB) provides the best anti-reversion performance for compound cured at 150°C, with N,N′-p-phenylene-biscitraconimide (BCpB) following closely behind. Although Perkalink 900 (1,3-bis(citraconimidomethyl)benzene: BCDB), 1,3-bis(citraconimido)isobutane (BIB), and 1,6-bis(citraconimido)hexane (BCH) are less effective than BCmB and BCpB in improving the anti-reversion performance of compound cured for a short period of time or cured at 150°C, they show better anti-reversion performance of compound cured for a longer time or cured at higher vulcanization temperature.
不同双柠檬酸亚胺在天然橡胶中抗逆转剂的比较研究
硫化天然橡胶(NR)在硫化过程中通常会发生还原反应,严重影响橡胶制品的性能和使用寿命。引入抗逆转剂是对抗逆转最有效的方法之一。本文合成了五种结构不同的双柠檬酸亚胺,并将其作为硫固化NR的抗还原剂。详细研究了抗还原剂在硫化特性、交联结构、物理力学性能、热积累和动态力学性能方面的差异,以阐述抗还原剂在反应性和交联化学方面的差异。结果表明,在150℃固化时,N,N′-对苯-双曲康酰亚胺(BCmB)的抗逆转性能最好,其次是N,N′-对苯-双曲康酰亚胺(BCpB)。虽然Perkalink 900(1,3-二(citraconimidom甲基)苯:BCDB)、1,3-二(citraconimido)异丁烷(BIB)和1,6-二(citraconimido)己烷(BCH)在提高短时间固化或150℃固化的复合材料的抗还原性能方面不如BCmB和BCpB,但它们在较长时间固化或较高硫化温度固化的复合材料中表现出更好的抗还原性能。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信