Jinfeng Zhao, D. Gamzina, A. Baig, L. Barnett, Jian-xun Wang, N. Luhmann
{"title":"Scandate dispenser cathode for 220 GHz 50W sheet beam travelling wave tube amplifier","authors":"Jinfeng Zhao, D. Gamzina, A. Baig, L. Barnett, Jian-xun Wang, N. Luhmann","doi":"10.1109/IRMMW-THZ.2011.6104761","DOIUrl":null,"url":null,"abstract":"Nanocomposite Sc2O3-added tungsten dispenser cathodes were tested in Cathode Life Test Vehicles (CLTV) with a Pierce gun configuration under CW mode. The emission performance for both dc and pulsed current density remained consistent. In CLTV #1, owing to perveance issue (there is 100 micron gap between focus electrode and cathode emission surface), 10 A/cm2 dc current density can be acquired at practical temperature of 1120°C Br for more than 2000 hours. In CLTV #2 with reduced FE gap, 45 A/cm2 dc current density is obtained.","PeriodicalId":6353,"journal":{"name":"2011 International Conference on Infrared, Millimeter, and Terahertz Waves","volume":"138 1","pages":"1-2"},"PeriodicalIF":0.0000,"publicationDate":"2011-12-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2011 International Conference on Infrared, Millimeter, and Terahertz Waves","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/IRMMW-THZ.2011.6104761","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2
Abstract
Nanocomposite Sc2O3-added tungsten dispenser cathodes were tested in Cathode Life Test Vehicles (CLTV) with a Pierce gun configuration under CW mode. The emission performance for both dc and pulsed current density remained consistent. In CLTV #1, owing to perveance issue (there is 100 micron gap between focus electrode and cathode emission surface), 10 A/cm2 dc current density can be acquired at practical temperature of 1120°C Br for more than 2000 hours. In CLTV #2 with reduced FE gap, 45 A/cm2 dc current density is obtained.