{"title":"Effect of mechanical activation and combustion parameters on titanium carbide SHS compaction","authors":"Yu. V. Bogatov, V. Shcherbakov","doi":"10.17073/1997-308x-2021-3-34-42","DOIUrl":null,"url":null,"abstract":"The paper presents the results of a study on the dense titanium carbide production by SHS compaction. It is shown that the use of a mechanically activated reaction mixture of titanium and carbon black powders makes it possible to obtain titanium carbide samples with a maximum relative density of 95 %. A feature of this research is that the mechanical activation of components and Ti + C mixture stirring were carried out in a ball mill. The study covers the influence of process parameters on the combustion properties and structure of the consolidated titanium carbide. It was found that the high-speed reaction mixture combustion is an essential condition for dense titanium carbide production. It was shown that the burning rate and temperature strongly depend on the size, mass and density of charge compacts. With an increase in the diameter (20–58 mm) and weight (10–70 g) of compacts made of mixtures with activated reagents, the burning rate varied from 10 to 100 cm/s, and the burning temperature varied from 2200 to 3100 °C. An influence of the pre-pressing pressure (applied at the combustion stage) on the burning rate and temperature was shown: the burning rate sharply decreases from 100 to 10 cm/s at pressures between 0 and 10 MPa, and the combustion temperature decreases monotonically from 3000 to 2000 °C at pressures between 0 and 40 MPa. A high-speed combustion mechanism was proposed for the titanium and carbon black reaction mixture where the formation of radial (longitudinal) cracks in compacts pressed from the mechanically activated mixture is an important factor. These cracks ensure the propagation of incandescent impurity gases and the exothermic reaction initiation in the sample volume.","PeriodicalId":14693,"journal":{"name":"Izvestiya vuzov. Poroshkovaya metallurgiya i funktsional’nye pokrytiya","volume":"9 16 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2021-09-17","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Izvestiya vuzov. Poroshkovaya metallurgiya i funktsional’nye pokrytiya","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17073/1997-308x-2021-3-34-42","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

The paper presents the results of a study on the dense titanium carbide production by SHS compaction. It is shown that the use of a mechanically activated reaction mixture of titanium and carbon black powders makes it possible to obtain titanium carbide samples with a maximum relative density of 95 %. A feature of this research is that the mechanical activation of components and Ti + C mixture stirring were carried out in a ball mill. The study covers the influence of process parameters on the combustion properties and structure of the consolidated titanium carbide. It was found that the high-speed reaction mixture combustion is an essential condition for dense titanium carbide production. It was shown that the burning rate and temperature strongly depend on the size, mass and density of charge compacts. With an increase in the diameter (20–58 mm) and weight (10–70 g) of compacts made of mixtures with activated reagents, the burning rate varied from 10 to 100 cm/s, and the burning temperature varied from 2200 to 3100 °C. An influence of the pre-pressing pressure (applied at the combustion stage) on the burning rate and temperature was shown: the burning rate sharply decreases from 100 to 10 cm/s at pressures between 0 and 10 MPa, and the combustion temperature decreases monotonically from 3000 to 2000 °C at pressures between 0 and 40 MPa. A high-speed combustion mechanism was proposed for the titanium and carbon black reaction mixture where the formation of radial (longitudinal) cracks in compacts pressed from the mechanically activated mixture is an important factor. These cracks ensure the propagation of incandescent impurity gases and the exothermic reaction initiation in the sample volume.
机械活化和燃烧参数对碳化钛SHS压实的影响
本文介绍了用SHS压实法生产致密碳化钛的研究结果。结果表明,使用钛粉和炭黑粉的机械活化反应混合物,可以得到最大相对密度为95%的碳化钛样品。本研究的一个特点是在球磨机中进行了组分的机械活化和Ti + C混合物的搅拌。研究了工艺参数对固结碳化钛燃烧性能和组织的影响。发现高速反应混合燃烧是生产致密碳化钛的必要条件。结果表明,燃烧速率和温度与装药块的大小、质量和密度密切相关。随着与活性剂混合制成的压坯直径(20 ~ 58 mm)和重量(10 ~ 70 g)的增加,燃烧速度在10 ~ 100 cm/s之间变化,燃烧温度在2200 ~ 3100℃之间变化。结果表明,预压压力(在燃烧阶段施加)对燃烧速度和温度的影响:在0 ~ 10 MPa压力范围内,燃烧速度从100 ~ 10 cm/s急剧下降;在0 ~ 40 MPa压力范围内,燃烧温度从3000℃单调下降到2000℃。提出了一种钛炭黑混合反应的高速燃烧机理,其中由机械活化的混合反应压下的压坯中形成径向(纵向)裂纹是一个重要因素。这些裂纹保证了白炽杂质气体的传播和样品体积中放热反应的开始。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信