{"title":"THE TEARING STRENGTH ANALYSIS OFDENIM FABRICS WITH \nDIFFERENT WEFT YARN TYPE AND WEFT YARN LAYOUT","authors":"M. Avcı, E. Sarıoğlu, G. K. Günaydin","doi":"10.35530/tt.2019.27","DOIUrl":null,"url":null,"abstract":"Denim fabrics which are highly demanded products among the world have high consumption rate in \nthe textile market. Those fabrics may be utilized for different purposes. Durability, elasticity, wearing\nresistance are the important expected properties from denim fabrics. Tearing resistance of denim fabrics in use is \nanother parameter that should be considered. This study includes the investigation of tearing properties of \ndenim fabrics produced from single core (Polyethylene terephthalate/Polytrimethylene terephthalate (PET/PTT) \nbicomponent filament and elastane) and dual core (PET/PTT+elastane feeding simultaneously) spun yarns \nutilized as weft yarns. Denim fabrics with different layout of these weft yarns with uncovered PET/PTT \nbicomponent filament were produced in order to compare the tearing strength properties in warp and weft wise. \nResults revealed that highest tearing strength of weft wise was obtained from denim fabrics at 2F:2CY layout \nwhere two uncovered PET/PTT bicomponent filament and two PET/PTT bicomponent filament+elastane dual \ncore-spun yarn were used consecutively in the layouts. The lowest tearing strength was found among the denim \nfabrics at 1F:6CY layout where one uncovered PET/PTT bicomponent filament and six PET/PTT bicomponent \nfilament+elastane dual core-spun yarns were used consecutively in the layouts. According to statistical \nevaluation; Weft yarn type, weft yarn layout and their interaction in the fabric were found to having significant \neffects on tearing strength for both warp and weft direction of denim fabric at significance level of 0.05.","PeriodicalId":22214,"journal":{"name":"TEXTEH Proceedings","volume":"21 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-11-05","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"TEXTEH Proceedings","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.35530/tt.2019.27","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
Denim fabrics which are highly demanded products among the world have high consumption rate in
the textile market. Those fabrics may be utilized for different purposes. Durability, elasticity, wearing
resistance are the important expected properties from denim fabrics. Tearing resistance of denim fabrics in use is
another parameter that should be considered. This study includes the investigation of tearing properties of
denim fabrics produced from single core (Polyethylene terephthalate/Polytrimethylene terephthalate (PET/PTT)
bicomponent filament and elastane) and dual core (PET/PTT+elastane feeding simultaneously) spun yarns
utilized as weft yarns. Denim fabrics with different layout of these weft yarns with uncovered PET/PTT
bicomponent filament were produced in order to compare the tearing strength properties in warp and weft wise.
Results revealed that highest tearing strength of weft wise was obtained from denim fabrics at 2F:2CY layout
where two uncovered PET/PTT bicomponent filament and two PET/PTT bicomponent filament+elastane dual
core-spun yarn were used consecutively in the layouts. The lowest tearing strength was found among the denim
fabrics at 1F:6CY layout where one uncovered PET/PTT bicomponent filament and six PET/PTT bicomponent
filament+elastane dual core-spun yarns were used consecutively in the layouts. According to statistical
evaluation; Weft yarn type, weft yarn layout and their interaction in the fabric were found to having significant
effects on tearing strength for both warp and weft direction of denim fabric at significance level of 0.05.