M. Theelen, M. Tomassini, N. Barreau, H. Steijvers, A. Branca, S. Harel, Z. Vroon, M. Zeman
{"title":"The impact of selenisation on damp heat degradation of the CIGS back contact molybdenum","authors":"M. Theelen, M. Tomassini, N. Barreau, H. Steijvers, A. Branca, S. Harel, Z. Vroon, M. Zeman","doi":"10.1109/PVSC-VOL2.2012.6656703","DOIUrl":null,"url":null,"abstract":"Molybdenum (Mo) degrades under the influence of damp heat, thereby reducing the output of CIGS PV. In this study, Mo layers were deposited on a glass substrate by magnetron sputtering, thereby varying the deposition pressure and the addition of selenium. These samples were thoroughly analysed and degraded at 60oC/60% relative humidity (RH) and 85°C /85% RH.","PeriodicalId":6420,"journal":{"name":"2012 IEEE 38th Photovoltaic Specialists Conference (PVSC) PART 2","volume":"21 1","pages":"1-6"},"PeriodicalIF":0.0000,"publicationDate":"2013-11-07","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"8","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2012 IEEE 38th Photovoltaic Specialists Conference (PVSC) PART 2","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/PVSC-VOL2.2012.6656703","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 8
Abstract
Molybdenum (Mo) degrades under the influence of damp heat, thereby reducing the output of CIGS PV. In this study, Mo layers were deposited on a glass substrate by magnetron sputtering, thereby varying the deposition pressure and the addition of selenium. These samples were thoroughly analysed and degraded at 60oC/60% relative humidity (RH) and 85°C /85% RH.