{"title":"Fracture Toughness Testing of an Overmatched Pipe Girth Weld Using Clamped SE(T) Specimens","authors":"C. Ferreira, D. Burgos, C. Ruggieri","doi":"10.1115/pvp2019-93256","DOIUrl":null,"url":null,"abstract":"\n This work presents an investigation of the ductile tearing properties for a girth weld made of an ASTM A106 Gr C steel using the SMAW welding process with a low hydrogen E7018 electrode thereby resulting in a weld with high strength overmatching with respect to the base material. Testing of the pipe girth welds employed side-grooved, clamped SE(T) specimens with a weld centerline notch to determine the crack growth resistance curves based upon the unloading compliance (UC) method using a single specimen technique. Recently developed compliance functions and η-factors applicable to weld centerline notched SE(T) specimens are introduced to determine crack growth resistance data from laboratory measurements of load-displacement records. While the UC procedure resulted in measured crack extensions for the tested specimens with weld centerline notch that underestimated the 9-point average crack extension, our preliminary results demonstrate the capability of the methodology in describing crack growth resistance behavior which serves as a basis for ductile tearing assessments in ECA procedures applicable to overmatched girth welds and similar structural components.","PeriodicalId":23651,"journal":{"name":"Volume 6B: Materials and Fabrication","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2019-11-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Volume 6B: Materials and Fabrication","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1115/pvp2019-93256","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
This work presents an investigation of the ductile tearing properties for a girth weld made of an ASTM A106 Gr C steel using the SMAW welding process with a low hydrogen E7018 electrode thereby resulting in a weld with high strength overmatching with respect to the base material. Testing of the pipe girth welds employed side-grooved, clamped SE(T) specimens with a weld centerline notch to determine the crack growth resistance curves based upon the unloading compliance (UC) method using a single specimen technique. Recently developed compliance functions and η-factors applicable to weld centerline notched SE(T) specimens are introduced to determine crack growth resistance data from laboratory measurements of load-displacement records. While the UC procedure resulted in measured crack extensions for the tested specimens with weld centerline notch that underestimated the 9-point average crack extension, our preliminary results demonstrate the capability of the methodology in describing crack growth resistance behavior which serves as a basis for ductile tearing assessments in ECA procedures applicable to overmatched girth welds and similar structural components.
本文研究了采用低氢E7018焊条进行SMAW焊接的ASTM A106 Gr C钢环焊缝的韧性撕裂性能,从而获得了与基材相匹配的高强度焊缝。采用带焊缝中心线缺口的侧槽夹紧SE(T)试样对管道环焊缝进行测试,采用单试样技术基于卸载依从性(UC)方法确定裂纹扩展阻力曲线。引入了最近开发的适用于焊缝中心线缺口SE(T)试样的柔度函数和η因子,以确定实验室测量的载荷-位移记录的裂纹扩展阻力数据。虽然UC程序导致了带有焊缝中心线缺口的测试样品的裂纹扩展测量,低估了9点的平均裂纹扩展,但我们的初步结果证明了该方法在描述裂纹扩展阻力行为方面的能力,该方法可作为适用于超匹配环焊缝和类似结构部件的ECA程序中韧性撕裂评估的基础。