Analysis on Degradation in Creep Strength of 9Cr-W Martensitic Steel

M. Tamura
{"title":"Analysis on Degradation in Creep Strength of 9Cr-W Martensitic Steel","authors":"M. Tamura","doi":"10.5539/jmsr.v10n1p1","DOIUrl":null,"url":null,"abstract":"In order to clarify the creep mechanism of high Cr martensitic steel, creep curves of 9Cr-1W and 9Cr-4W steels were analyzed applying an exponential law to the temperature, stress, and time parameters. The activation energy, Q, the activation volume, V, and the Larson-Miller constant, C, are obtained as functions of creep strain. At the beginning of creep, sub-grain boundary strengthening by swept dislocations out of sub-grains occurs followed by strengthening due to the rearrangement of M23C6 and the precipitation of Laves phase. After Q reaches a peak, heterogeneous recovery and subsequent heterogeneous deformation begin at an early stage of transient creep in the vicinity of some weakest boundaries due to coarsening of the precipitates, which triggers the unexpected degradation in strength due to the accelerating coarsening of precipitates. Stabilizing not only M23C6 but also Laves phase is important to mitigate the degradation of rupture strength of martensitic steel. The above creep mechanism for martensitic steel can be applicable to the explanation for the degradation in long term rupture strength of high Cr martensitic steel, Grades 91 and 92.","PeriodicalId":16111,"journal":{"name":"Journal of Materials Science Research","volume":"362 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2021-06-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Materials Science Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5539/jmsr.v10n1p1","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

Abstract

In order to clarify the creep mechanism of high Cr martensitic steel, creep curves of 9Cr-1W and 9Cr-4W steels were analyzed applying an exponential law to the temperature, stress, and time parameters. The activation energy, Q, the activation volume, V, and the Larson-Miller constant, C, are obtained as functions of creep strain. At the beginning of creep, sub-grain boundary strengthening by swept dislocations out of sub-grains occurs followed by strengthening due to the rearrangement of M23C6 and the precipitation of Laves phase. After Q reaches a peak, heterogeneous recovery and subsequent heterogeneous deformation begin at an early stage of transient creep in the vicinity of some weakest boundaries due to coarsening of the precipitates, which triggers the unexpected degradation in strength due to the accelerating coarsening of precipitates. Stabilizing not only M23C6 but also Laves phase is important to mitigate the degradation of rupture strength of martensitic steel. The above creep mechanism for martensitic steel can be applicable to the explanation for the degradation in long term rupture strength of high Cr martensitic steel, Grades 91 and 92.
9Cr-W马氏体钢蠕变强度退化分析
为了阐明高铬马氏体钢的蠕变机理,应用温度、应力和时间参数的指数规律对9Cr-1W和9Cr-4W钢的蠕变曲线进行了分析。得到了活化能Q、活化体积V和Larson-Miller常数C作为蠕变应变的函数。在蠕变开始时,由亚晶外扫位错强化亚晶界,然后由M23C6的重排和Laves相的析出强化亚晶界。在Q达到峰值后,非均质恢复和随后的非均质变形开始于瞬态蠕变的早期阶段,在一些因析出相粗化而最弱的边界附近,这导致了由于析出相加速粗化而导致的意外强度退化。稳定M23C6相和Laves相对减缓马氏体钢断裂强度下降具有重要意义。上述马氏体钢蠕变机理可用于91级和92级高铬马氏体钢长期断裂强度下降的解释。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信