Strength Development and Lateral Load Resisting Properties of Expanded Polystyrene Based Lightweight Concrete Panels

IF 0.4 Q4 ENGINEERING, MULTIDISCIPLINARY
S. Sivakanthan, P. N. Karandeniya, B. E. Thevarajah, M. Jayasinghe
{"title":"Strength Development and Lateral Load Resisting Properties of Expanded Polystyrene Based Lightweight Concrete Panels","authors":"S. Sivakanthan, P. N. Karandeniya, B. E. Thevarajah, M. Jayasinghe","doi":"10.4038/engineer.v55i3.7524","DOIUrl":null,"url":null,"abstract":": The construction industry is rapidly moving toward sustainable development due to the rise of the scarcity of natural resources and the climatic impact on the environment. Several studies have been carried out related to the subject of Expanded Polystyrene (EPS) based lightweight concrete panel production and its usages in buildings. This paper mainly focuses on strength development and lateral load-bearing capacity of the EPS panels where these panels are used as a loadbearing wall in buildings. Lateral loading resistance properties and performance of lightweight wall panels were assessed by carrying out load tests on scale down wall specimens representing the actual wall construction. The strength development of EPS-based concrete panels was assessed by developing strength curves from compressive strength tests carried out for different curing conditions of the lightweight concrete. The outcomes of this study show that the flexural strength parallel to the wall panels is in the range of 0.58 to 0.70N/mm 2 . Under wet conditions, it reduces to 0.45 N/mm 2 . Also, there was an average of 0.4 N/mm 2 compressive strength difference between properly cured and non-cured EPS samples, which is approximately 20% of strength development in the six month period.","PeriodicalId":42812,"journal":{"name":"Engineer-Journal of the Institution of Engineers Sri Lanka","volume":"9 1","pages":""},"PeriodicalIF":0.4000,"publicationDate":"2022-11-08","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Engineer-Journal of the Institution of Engineers Sri Lanka","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4038/engineer.v55i3.7524","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"ENGINEERING, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

Abstract

: The construction industry is rapidly moving toward sustainable development due to the rise of the scarcity of natural resources and the climatic impact on the environment. Several studies have been carried out related to the subject of Expanded Polystyrene (EPS) based lightweight concrete panel production and its usages in buildings. This paper mainly focuses on strength development and lateral load-bearing capacity of the EPS panels where these panels are used as a loadbearing wall in buildings. Lateral loading resistance properties and performance of lightweight wall panels were assessed by carrying out load tests on scale down wall specimens representing the actual wall construction. The strength development of EPS-based concrete panels was assessed by developing strength curves from compressive strength tests carried out for different curing conditions of the lightweight concrete. The outcomes of this study show that the flexural strength parallel to the wall panels is in the range of 0.58 to 0.70N/mm 2 . Under wet conditions, it reduces to 0.45 N/mm 2 . Also, there was an average of 0.4 N/mm 2 compressive strength difference between properly cured and non-cured EPS samples, which is approximately 20% of strength development in the six month period.
膨胀聚苯乙烯基轻质混凝土板的强度发展及抗侧载性能
由于自然资源的稀缺和气候对环境的影响,建筑行业正在迅速走向可持续发展。关于以聚苯乙烯(EPS)为基础的轻质混凝土板的生产及其在建筑中的应用进行了一些研究。本文主要研究EPS板作为建筑承重墙的强度发展和侧向承载能力。通过对代表实际墙体结构的按比例缩小的墙体试件进行荷载试验,评估了轻质墙板的抗侧载性能和性能。通过对轻量化混凝土不同养护条件下的抗压强度试验绘制强度曲线,对eps基混凝土板的强度发展进行了评价。研究结果表明,平行于墙板的抗弯强度在0.58 ~ 0.70N/mm 2之间。在潮湿条件下,它降低到0.45 N/ mm2。此外,适当固化和未固化EPS样品之间的平均抗压强度差异为0.4 N/mm 2,约为六个月期间强度发展的20%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
38
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信