{"title":"Recovery Process for Critical Metals: Selective Adsorption of Nickel(II) from Cobalt(II) at Acidic Condition and Elevated Temperature","authors":"Friederike Kriese, S. Lassen, B. Niemeyer","doi":"10.1155/2023/5334353","DOIUrl":null,"url":null,"abstract":"Effective and sustainable separation processes for critical metals, especially for the physicochemically similar elements nickel and cobalt in battery recycling, are of great interest in the future. Selective adsorption represents a highly potential process for this purpose. In this publication, a silica adsorbent functionalized with an amino-polycarboxylate derivate (HSU331) was investigated regarding the selective adsorption of Ni(II) in the presence of Co(II) in acidic solution (pH range at equilibrium 1.8–2.3) at elevated temperature. Comparable maximum equilibrium loadings (\n \n \n \n q\n \n \n max\n \n \n \n ) for Ni(II) and Co(II) of 0.59 μmol(Ni(II)) · μmol(Ligand)-1 (18.3 mg(Ni(II)) · g(Adsorbent)-1), and 0.52 μmol(Co(II)) · μmol(Ligand)-1 (16.0 mg(Co(II)) · g(Adsorbent)-1), respectively, were achieved at T = 50°C in single-component experiments. Under competitive conditions, the Ni(II) loading remained constant at 0.60 μmol(Ni(II)) · μmol(Ligand)-1 (18.4 mg(Ni(II)) · g(Adsorbent)-1), while the Co(II) loading drastically decreased to 0.09 μmol(Co(II)) · μmol(Ligand)-1 (2.7 mg(Co(II)) · g(Adsorbent)-1) in an equimolar dual-component system. Calculated stability constants of 3 · 103 and 0.7 · 103 L · mol-1, respectively, for the formed metal ion complexes of Ni(II) and Co(II) onto the adsorbent HSU331, clarify the clear selectivity of the adsorbent towards Ni(II) in the presence of Co(II) even at elevated temperature (T = 50°C).","PeriodicalId":7279,"journal":{"name":"Adsorption Science & Technology","volume":"21 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-02-03","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Adsorption Science & Technology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1155/2023/5334353","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

Abstract

Effective and sustainable separation processes for critical metals, especially for the physicochemically similar elements nickel and cobalt in battery recycling, are of great interest in the future. Selective adsorption represents a highly potential process for this purpose. In this publication, a silica adsorbent functionalized with an amino-polycarboxylate derivate (HSU331) was investigated regarding the selective adsorption of Ni(II) in the presence of Co(II) in acidic solution (pH range at equilibrium 1.8–2.3) at elevated temperature. Comparable maximum equilibrium loadings ( q max ) for Ni(II) and Co(II) of 0.59 μmol(Ni(II)) · μmol(Ligand)-1 (18.3 mg(Ni(II)) · g(Adsorbent)-1), and 0.52 μmol(Co(II)) · μmol(Ligand)-1 (16.0 mg(Co(II)) · g(Adsorbent)-1), respectively, were achieved at T = 50°C in single-component experiments. Under competitive conditions, the Ni(II) loading remained constant at 0.60 μmol(Ni(II)) · μmol(Ligand)-1 (18.4 mg(Ni(II)) · g(Adsorbent)-1), while the Co(II) loading drastically decreased to 0.09 μmol(Co(II)) · μmol(Ligand)-1 (2.7 mg(Co(II)) · g(Adsorbent)-1) in an equimolar dual-component system. Calculated stability constants of 3 · 103 and 0.7 · 103 L · mol-1, respectively, for the formed metal ion complexes of Ni(II) and Co(II) onto the adsorbent HSU331, clarify the clear selectivity of the adsorbent towards Ni(II) in the presence of Co(II) even at elevated temperature (T = 50°C).
临界金属的回收工艺:酸性和高温条件下镍(II)从钴(II)中选择性吸附
有效和可持续的分离关键金属的过程,特别是物理化学相似的元素镍和钴在电池回收,是未来的极大兴趣。选择性吸附是实现这一目的的一种极具潜力的方法。在这篇论文中,研究了一种氨基聚羧酸衍生物(HSU331)功能化的二氧化硅吸附剂在Co(II)存在下在酸性溶液(pH值范围为1.8-2.3)中在高温下对Ni(II)的选择性吸附。在单组分实验中,温度为50℃时,Ni(II)和Co(II)的最大平衡负荷(q max)分别为0.59 μmol(Ni(II))·μmol(配体)-1 (18.3 mg(Ni(II))·g(吸附剂)-1)和0.52 μmol(Co(II))·μmol(配体)-1 (16.0 mg(Co(II))·g(吸附剂)-1)。在竞争条件下,在等摩尔双组分体系中,Ni(II)的负载量保持在0.60 μmol(Ni(II))·μmol(配体)-1 (18.4 mg(Ni(II))·g(吸附剂)-1),而Co(II)的负载量急剧下降至0.09 μmol(Co(II))·μmol(配体)-1 (2.7 mg(Co(II))·g(吸附剂)-1)。计算出在吸附剂HSU331上形成的Ni(II)和Co(II)金属离子配合物的稳定性常数分别为3·103和0.7·103 L·mol-1,阐明了吸附剂在Co(II)存在下即使在高温(T = 50℃)下对Ni(II)的明显选择性。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信