{"title":"Фронтальный контакт к GaSb-фотопреобразователям: свойства и температурная стабильность","authors":"С.В. Сорокина, Ф.Ю. Солдатенков, Н.С. Потапович, В.П. Хвостиков","doi":"10.21883/ftp.2023.01.54928.3692","DOIUrl":null,"url":null,"abstract":"Issues related to the thermal stability of front contacts, based on Cr-Au and Cr-Au-Ag-Au, to GaSb-based photovoltaic cells have been considered at the operational (the cell temperature is 50 oC) and standard conditions as well as at the forced thermal degradation (at 125 and 200 oC). It is shown that the photovoltaic converter with the silver-containing contact is preferable in terms of the stability of contact resistivity, external quantum yield, FF, VOC, and therefore, the cell efficiency and lifetime. The durability of the cells is determined at operational and elevated temperatures.","PeriodicalId":24054,"journal":{"name":"Физика и техника полупроводников","volume":"23 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Физика и техника полупроводников","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.21883/ftp.2023.01.54928.3692","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
Issues related to the thermal stability of front contacts, based on Cr-Au and Cr-Au-Ag-Au, to GaSb-based photovoltaic cells have been considered at the operational (the cell temperature is 50 oC) and standard conditions as well as at the forced thermal degradation (at 125 and 200 oC). It is shown that the photovoltaic converter with the silver-containing contact is preferable in terms of the stability of contact resistivity, external quantum yield, FF, VOC, and therefore, the cell efficiency and lifetime. The durability of the cells is determined at operational and elevated temperatures.
基于Cr-Au和Cr-Au- ag - au的前触点与gasb基光伏电池的热稳定性有关的问题已经在操作(电池温度为50℃)和标准条件下以及在强制热降解(125℃和200℃)下被考虑。结果表明,在接触电阻率、外量子产率、FF和VOC的稳定性以及电池效率和寿命方面,含银触点的光伏变换器具有较好的稳定性。电池的耐久性取决于操作温度和高温。