{"title":"Characterization of MCM-41 Mesoporous Silica Supported 2-Carboxyethyl Phenyl Phosphinic Acid","authors":"Z. Han, Feng Xu, Li Jiang, Z. Jiang, Peng Wang","doi":"10.4028/www.scientific.net/KEM.591.134","DOIUrl":null,"url":null,"abstract":"MCM-41 mesoporous silica was prepared by hydrothermal method. 2-carboxyethyl phenyl phosphinic acid (CEPPA) was loaded on MCM-41 by solution method. The structure of MCM-41 and its supported CEPPA was studied by X-ray diffraction (XRD), transmission electron microscope (TEM) and scanning electron microscopy (SEM) coupled with energy dispersive spectrometer (EDS). The results revealed that CEPPA was successfully loaded on MCM-41 with Si/P molar ratio of about 20:1. The XRD spectrum of MCM-41 supported CEPPA was different from MCM-41, indicating the structure of MCM-41 was changed after loading of CEPPA. CEPPA molecule moved into the mesoporous structure and filled in the mesopores, leading to the disappearance of characteristic diffraction peaks of MCM-41. The interaction between hydroxyl group of CEPPA and silanol of MCM-41 made it stable for CEPPA to be in the mesopores and on the surface of MCM-41. MCM-41 supported CEPPA also showed the similar mesoporous structure with long-range order to MCM-41 when observed by TEM. SEM provided further evidences of the similar particle size and different morphology.","PeriodicalId":17714,"journal":{"name":"Key Engineering Materials","volume":"23 1","pages":"134 - 137"},"PeriodicalIF":0.0000,"publicationDate":"2013-11-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Key Engineering Materials","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4028/www.scientific.net/KEM.591.134","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
MCM-41 mesoporous silica was prepared by hydrothermal method. 2-carboxyethyl phenyl phosphinic acid (CEPPA) was loaded on MCM-41 by solution method. The structure of MCM-41 and its supported CEPPA was studied by X-ray diffraction (XRD), transmission electron microscope (TEM) and scanning electron microscopy (SEM) coupled with energy dispersive spectrometer (EDS). The results revealed that CEPPA was successfully loaded on MCM-41 with Si/P molar ratio of about 20:1. The XRD spectrum of MCM-41 supported CEPPA was different from MCM-41, indicating the structure of MCM-41 was changed after loading of CEPPA. CEPPA molecule moved into the mesoporous structure and filled in the mesopores, leading to the disappearance of characteristic diffraction peaks of MCM-41. The interaction between hydroxyl group of CEPPA and silanol of MCM-41 made it stable for CEPPA to be in the mesopores and on the surface of MCM-41. MCM-41 supported CEPPA also showed the similar mesoporous structure with long-range order to MCM-41 when observed by TEM. SEM provided further evidences of the similar particle size and different morphology.