Y. Bae, I. Um
{"title":"Effect of addition of methanol on rheological properties of silk formic acid solution","authors":"Y. Bae, I. Um","doi":"10.7852/IJIE.2020.40.1.28","DOIUrl":null,"url":null,"abstract":"Recently, many studies have been undertaken on the wet spinning and electrospinning of silk because wet-spun fibers and electrospun webs of silk can be applied in the biomedical and cosmetic fields owing to the good biocompatibility of silk. The rheological properties of silk solution are important because they strongly affect the spinning performance of the silk solution and the structures of resultant fibrous materials. Therefore, as a preliminary study on the effect of solvent composition on the rheological properties of silk fibroin (SF) solution and structure of the resultant film, in the reported work, methanol was added to the SF formic acid solution. A small amount of methanol (i.e. 2%) added to the SF formic acid solution significantly altered the rheological properties of the solution: its shear viscosity increased by 10 folds at low shear and decreased on increasing the shear rate, demonstrating shear thinning behavior of the SF solution. Dynamic tests for the SF solution indicated that the addition of 2% methanol altered the viscous state of the SF formic acid solution to elastic. However, the molecular conformation (i.e. β-sheet conformation) of the regenerated SF film cast from formic acid remained unchanged on the addition of 2% methanol. © 2020 The Korean Society of Sericultural Sciences Int. J. Indust. Entomol. 40(1), 28-32 (2020)","PeriodicalId":14140,"journal":{"name":"International journal of industrial entomology","volume":"51 1","pages":"28-32"},"PeriodicalIF":0.0000,"publicationDate":"2020-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International journal of industrial entomology","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.7852/IJIE.2020.40.1.28","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
甲醇的加入对丝甲酸溶液流变性能的影响
由于蚕丝具有良好的生物相容性,湿纺纤维和静电纺丝网可用于生物医学和化妆品领域,近年来,人们对蚕丝的湿纺和静电纺丝进行了大量的研究。丝液的流变性能对丝液的纺丝性能和纤维材料的结构产生重要的影响。因此,为了初步研究溶剂组成对丝素(SF)溶液流变性能和所得膜结构的影响,本文在丝素甲酸溶液中加入甲醇。在SF甲酸溶液中加入少量甲醇(即2%),显著改变了溶液的流变性能:在低剪切时,其剪切粘度增加10倍,随着剪切速率的增加而降低,表明SF溶液具有剪切变薄的行为。动态实验表明,加入2%甲醇后,SF甲酸溶液的粘性状态变为弹性状态。然而,在添加2%甲醇的情况下,甲酸浇铸的再生SF膜的分子构象(即β-片状构象)保持不变。©2020韩国蚕桑科学学会。j .的尘埃。昆虫学报,40(1),28-32 (2020)
本文章由计算机程序翻译,如有差异,请以英文原文为准。